Carrier-induced dynamic strain effects in semiconductor nanocrystals Xue-Shu ZhaoYu-Ru GeXin Zhao OriginalPaper Pages: 4267 - 4285
Effects of HF treatments on tensile strength of Hi-Nicalon fibres N. P. Bansal OriginalPaper Pages: 4287 - 4295
Sinterability of commercial 8 mol% yttria-stabilized zirconia powders and the effect of sintered density on the ionic conductivity I. R. GibsonG. P. DransfieldJ. T. S. Irvine OriginalPaper Pages: 4297 - 4305
Specimen size effects in the tensile failure strain of an epoxy adhesive A. TowseK. PotterR. D. Adams OriginalPaper Pages: 4307 - 4314
Hot-salt oxidation characteristics of titanium aluminides S. V. KumariJ. A. Little OriginalPaper Pages: 4315 - 4319
Sintering and microstructure development in the system MgO–TiO2 Y. B. LeeH. C. ParkF. L. Riley OriginalPaper Pages: 4321 - 4325
Preload relaxation of threaded fasteners in sand-castings of zinc-based alloys A. A. MirS. Murphy OriginalPaper Pages: 4327 - 4332
Chemical synthesis of the high-pressure cubic-spinel phase of ZnIn2S4 M. A. SriramP. H. McMichaelX.-L. Wang OriginalPaper Pages: 4333 - 4339
Investigation of the pyrolysis of lead zirconate titanate gels with coupled differential thermal analysis, thermogravimetry and infrared spectroscopy R. MerkleH. Bertagnolli OriginalPaper Pages: 4341 - 4348
Biaxial monotonic and fatigue fracture of some commercial ABS and PVC sheets A. G. AtkinsG. JeronimidisS. Arndt OriginalPaper Pages: 4349 - 4356
Hydrothermal degradation of chemical vapour deposited SiC fibres T. KraftK. G. NickelY. G. Gogotsi OriginalPaper Pages: 4357 - 4364
Effects of composition on microstructures of rapidly solidified Ni–Al alloys Tianyi ChengW. LÖserM. Leonhardt OriginalPaper Pages: 4365 - 4374
Discrete β-Ta2O5 crystallite formation in reactively sputtered amorphous thin films P. J. BeckageD. B. KnorrE. J. Rymaszewski OriginalPaper Pages: 4375 - 4379
Thermal expansion of isotropic Duralcan metal–matrix composites S. LemieuxS. ElomariM. D. Skibo OriginalPaper Pages: 4381 - 4387
Effect of martensitic transformation in Ti–15 at % V β-phase particles on lamellar boundary decohesion in γ-TiAl Part I Derivation of interface decohesion potentials M. GrujicicS. G. Lai OriginalPaper Pages: 4389 - 4400
Effect of martensitic transformation in Ti–15 at %V β-phase particles on lamellar boundary decohesion in γ-TiAl Part II Finite element analysis of crack-bridging phenomenon M. GrujicicS. G. Lai OriginalPaper Pages: 4401 - 4415
Spray deposition of an iron aluminide J. R. BlackfordR. A. BuckleyA. J. Horlock OriginalPaper Pages: 4417 - 4421
Microstructure and crystal structure development in porous titania coatings prepared from anhydrous titanium ethoxide solutions Y. J. KimL. F. Francis OriginalPaper Pages: 4423 - 4433
Effect of NiO and/or TiO2 mullite formation and microstructure from gels M. SalesJ. VilaJ. AlarcÖn OriginalPaper Pages: 4435 - 4446
Oxide and interface characteristics of oxidized silicon oxynitride ceramics – an investigation by electron microscopy D. ManessisHonghua DuR. Larker OriginalPaper Pages: 4447 - 4453
Sol-gel processed barium titanate ceramics and thin films H. B. SharmaA. Mansingh OriginalPaper Pages: 4455 - 4459
On the CVD of MoSi2: an experimental study from the MoCl4–SiCl4–H2–Ar precursor with a view to the preparation of C/MoSi2/SiC and SiC/MoSi2/SiC microcomposites J. L. BobetG. VignolesR. Naslain OriginalPaper Pages: 4461 - 4473