Effect of the shape and porous structure of the particles of an iron powder on its characteristics M. I. KononovYa. M. Turetskii OriginalPaper Pages: 521 - 523
Effect of electrolysis conditions on the formation, structure, and magnetic properties of a finely divided iron-cobalt alloy V. V. MyalkovskiiE. P. Zhelibo OriginalPaper Pages: 524 - 529
Coating tungsten carbide particles by cobalt electrodeposition V. M. ZanozinR. V. Rybal'chenkoYu. M. Polukarov OriginalPaper Pages: 529 - 533
Electrochemical production of tungsten-iron powders of predetermined composition B. P. Yur'evS. P. ShkuryakovaN. B. Maksimenko OriginalPaper Pages: 533 - 536
Calculation of the sintering parameters of viscous solids P. A. PavlovE. L. YakovlevaI. D. Fridberg OriginalPaper Pages: 537 - 539
Alloy formation during the sintering of molybdenum-chromium powder mixtures L. L. KolomietsS. M. Solonin OriginalPaper Pages: 540 - 544
An albedo electron method for measuring the density of P/M materials B. A. KononovV. N. RudenkoA. V. Sakhnenko OriginalPaper Pages: 545 - 548
Effective area of contact of reinforced plasma-sprayed coatings D. M. KarpinosV. G. Zil'berbergA. G. Il'enko OriginalPaper Pages: 549 - 552
High-porosity permeable materials from metal fibers A. G. KostornovA. L. Moroz OriginalPaper Pages: 553 - 556
Manufacture of small bearings from atomized powders Kh. I. ImanovT. N. KornevYu. I. Naida OriginalPaper Pages: 556 - 559
Structure and properties of fused single-crystal titanium carbide V. S. Sinel'nikovaT. I. ShtukaturovaV. A. Kuz'mishchev OriginalPaper Pages: 560 - 563
Effect of the surface structure of carbon fibers on their strength in the application of a carbide coating in a metal melt V. E. OvcharenkoO. A. KashinS. E. Salibekov OriginalPaper Pages: 564 - 567
Physicochemical reaction between fibers and a matrix in the hot pressing of an aluminum-boron composite material M. Kh. ShorshorovV. A. KolesnichenkoS. S. Dryunin OriginalPaper Pages: 567 - 570
Phase constitution and thermodynamic properties of alloys of the Mn-Si system in the range from 25 to 37.5 at. %Si G. M. LukashenkoV. R. SidorkoB. Ya. Kotur OriginalPaper Pages: 571 - 574
Method for increasing equipment utilization N. A. AkastelovaS. I. VdovinS. K. Senotrusov OriginalPaper Pages: 577 - 578
Morphology, microhardness, and grinding ability of single-crystal powders V. E. PopovYu. N. Vil'kT. M. Chekrygina OriginalPaper Pages: 578 - 581
Effect of sintering technology on the structure and properties of 20Kh13 martensitic-ferritic chromium steel V. A. DovydenkovI. D. Radomysel'skii OriginalPaper Pages: 582 - 585
X-ray diffraction investigation of the contact reactions of titanium-, vanadium-, and chromium-containing gallium melts with quartz and graphite V. G. ChuprinaYu. N. ChuvashovV. S. Zhuravlev OriginalPaper Pages: 585 - 588
Properties of plasma-deposited composite metal-boron nitride coatings F. I. KitaevYu. G. Lekarev OriginalPaper Pages: 589 - 593