Selection of optimum quenching parameters for large rotors of steel 25KhN3MFA I. A. Borisov Heat Treatment Technology Pages: 857 - 861
Transformations during high tempering in steel 25KhN3MFA A. Sh. Shneiderman Heat Treatment Technology Pages: 862 - 864
Strengthening mechanism of steel in tempering after surface plastic deformation E. A. Kurits Strength Properties Pages: 865 - 867
Features of the fatigue failure of steel with metastable austenite Yu. B. L'vovA. Ya. MaloletnevYa. B. Gurevich Strength Properties Pages: 868 - 870
Fracture of steel at different stages of hydrogen embrittlement É. A. SavchenkovA. F. Svetlichkin Strength Properties Pages: 871 - 876
Defects and long-term strength of materials with low deformability Yu. K. PetrenyaA. A. Chizhik Conference Materials Pages: 877 - 879
Microfracture of metals during high-temperature creep V. I. BetekhtinA. G. KadomtsevA. I. Petrov Conference Materials Pages: 879 - 881
Structure, defectiveness, and service life of heat-resistant steel during prolonged operation V. I. Kumanin Conference Materials Pages: 882 - 886
Operational reliability of high-pressure steam pipe made from pearlitic steels after operation for 150,000–200,000 h E. Ya. VekslerV. M. ChaikovskiiV. V. Osasyuk Conference Materials Pages: 886 - 889
Long-term strength of heat-resistant steels under creep conditions V. F. ZlepkoM. M. MelamedT. A. Shvetsova Conference Materials Pages: 889 - 892
Relationship between the maximum permissible creep strain and defectiveness of steam pipe materials T. G. BerezinaI. I. Trunin Conference Materials Pages: 892 - 895
High-temperature x-ray structural examination of steel R6M5 in the tempering process I. K. KupalovaE. M. Stepnov Technical Information Pages: 896 - 898
New corrosion-resistant steel, 16KhNKGMB-VI A. L. ShpitsbergV. A. Borisov Technical Information Pages: 898 - 899
Formation of amorphous phase in cast iron R. L. SnezhnoiA. A. ZhukovA. N. Kokora Technical Information Pages: 900 - 901
Effect of the composition and crystallization conditions on the properties and type of fracture of AZhN bronze I. I. ProkhorovM. P. ShebatinovN. A. Polushkin Technical Information Pages: 902 - 904
Diffusion of tin during growth of the Nb3Sn layer A. A. BochvarV. S. SergeevM. A. Fomishkin Technical Information Pages: 904 - 907
Structure of magnesium alloys with rare-earth metals M. V. ChukhrovZ. N. Khrisanova Technical Information Pages: 907 - 910
High-temperature transformation in magnetically hard iron — Chromium — Cobalt alloys N. I. MikheevA. A. Prozorov Technical Information Pages: 911 - 913