Examination of the dependence of adsorption of water and anions on metals on the potential by the contact electric resistance method V. A. Marichev OriginalPaper Pages: 123 - 131
Effect of the corrosive medium on propagation of short cracks J. EichemeyerF. Schlaet OriginalPaper Pages: 131 - 138
Effect of low temperature and medium on the kinetics of fatigue failure of 3M titanium alloy E. I. AleksenkoN. M. GrinbergG. I. Arkavenko OriginalPaper Pages: 138 - 144
Characteristics of damage of low-alloy steels in corrosion-active hydrogen sulfide-containing media T. V. TetyuevaL. R. BotvinaS. A. Krupnin OriginalPaper Pages: 144 - 149
Role of the high pressure of hydrogen in the phenomenon of hydrogen sulfide corrosion cracking of steel V. I. AlekseevO. A. KiselevI. V. Levshina OriginalPaper Pages: 149 - 152
Adsorption effect of liquid lithium on the mechanical properties of 12Kh12M2BFR steel A. V. VertkovV. A. EvtikhinA. A. Sychev OriginalPaper Pages: 153 - 156
Effect of hydrogen on the surface energy of metals Yu. I. KhomitskiiP. I. YukhnovskiiV. I. Tkachev OriginalPaper Pages: 156 - 159
High-temperature physicochemical interaction of titanium and its alloys with gas media V. N. Fedirko OriginalPaper Pages: 163 - 167
Accelerated corrosion cracking tests of steels in active-passive loading I. A. Muizhnek OriginalPaper Pages: 168 - 171
Effect of oxidation and sulfide corrosion in the conditions of a high-temperature gas flow on the strength characteristics of ÉI-958 alloy A. L. RozhkoV. P. LesnikovB. F. Rybalko OriginalPaper Pages: 172 - 175
Evaluation of the static cracking resistance of the metal calculating the critical defect size in bands of large compound support rolls O. N. RomanivYu. A. GrushkoV. N. Simin'kovich OriginalPaper Pages: 176 - 182
High-temperature cracking resistance in cast steel in reforming oven tubes G. M. NikiforchinO. Z. StudentS. I. Ripets'kii OriginalPaper Pages: 183 - 188
Brittle failure susceptibility of metal of a large structure S. V. SafronovV. G. BuduevaA. V. Klubochkin OriginalPaper Pages: 189 - 193
Variation of the properties of thin-walled shells of AMg6 alloy after long-term service V. G. KudryashovS. V. SafronovN. V. Tsikurenko OriginalPaper Pages: 194 - 197
Effect of damage in low-cycle fatigue on the speed of elastic waves V. V. Mishakin OriginalPaper Pages: 198 - 200
Simulating crack initiation and failure in a multilayer composite: Effective-strength distribution in a unidirectional reinforced composite M. V. Delyavs'kii OriginalPaper Pages: 201 - 205
Contact interaction between two half-spaces in the presence of a surface recess partially filled with an incompressible liquid R. M. Martinyak OriginalPaper Pages: 205 - 208
The electromagnetic field scattered by a crack in a piecewise-homogeneous medium: Theory of nondestructive testing Z. T. NazarchukO. I. Ovsyannikov OriginalPaper Pages: 208 - 213
Corrosion resistance of PT-3V titanium alloy and its welded joints in sulfide solutions V. E. BlashchukL. M. OnoprienkoV. É. Troyanovskii Science to Production Pages: 214 - 217
Efficiency of inhibitors in inhibiting corrosion and copper plating steel in acid solutions A. K. Mindyuk Science to Production Pages: 217 - 219
Wear resistance in steel 45 after frictional treatment by rubbing without seizure I. V. GureiYu. I. BabeiV. V. Shvets' Science to Production Pages: 220 - 222
Corrosion and strength behavior of aluminum in the formic acid-water system V. -I. D. Zaritskii Science to Production Pages: 223 - 225
Mechanism of formation of hot gas sprayed coatings on SCh-20 cast iron V. B. SapiroA. V. TsarevT. M. Duzhik Science to Production Pages: 225 - 227
Methods of determining the properties of corrosion cracking inhibitors V. M. KushnarenkoM. D. GetmanskiiB. D. Elemanov Science to Production Pages: 228 - 230
Acoustic emission inspection of stress corrosion of structural steels V. P. VoroninA. Yu. Shul'teV. I. Lukashenko Science to Production Pages: 230 - 233
Simulating anodic dissolution at the vertex of a crack growing in steps I. Z. DutsyakI. P. GnipE. I. Lichkovs'kii Science to Production Pages: 233 - 236
Effect of sludge of iron ore sinter on failure of pipe steels A. E. AndreikivM. V. Chernets Science to Production Pages: 236 - 242