Effect of transverse cracks on lamb wave velocity in CFRP cross-ply laminates Nobuyuki ToyamaTomonaga OkabeTeruo Kishi OriginalPaper Pages: 271 - 273
Synthesis and magnetic properties of a Fe-Ni alloy dispersed Al2O3 nanocomposite powder prepared by a chemical method Sung-Tag OhSeok NamkungJai-Sung Lee OriginalPaper Pages: 275 - 277
On substrate selection for direct ink-jet printing B. Y. TayM. J. Edirisinghe OriginalPaper Pages: 279 - 281
Direct comparison of the recoilless fractions in iron (II) and iron (III) chlorides using the two-lattice method M. Sorescu OriginalPaper Pages: 283 - 284
Characterization of copolymer poly(acrylonitrile) based polymer electrolytes H. P. ChenJ. W. FergusC. Shannon OriginalPaper Pages: 285 - 287
TEM study on domain configuration in LiTaO3 toughened Al2O3 ceramic composite Y. G. LiuY. ZhouZ. H. Huang OriginalPaper Pages: 289 - 291
Er3+ doped ultra-transparent oxy-fluoride glass-ceramics for application in the 1.54 μm telecommunication window V. K. TikhomirovD. FurnissR. Rolli OriginalPaper Pages: 293 - 295
Ferroelectric phase transition in calcium tellurite ceramics R. RaiS. SharmaR. N. P. Choudhary OriginalPaper Pages: 297 - 299
Triggered nucleation in Ni60Nb40 using an electrostatic levitator T. J. RathzM. B. RobinsonD. Li OriginalPaper Pages: 301 - 303
Adhesion between differently treated fibers and a hybrid resin system O. BrovkoP. RossoK. Friedrich OriginalPaper Pages: 305 - 308
Surface tension of pure aluminum in argon/hydrogen and nitrogen/hydrogen atmospheres at high temperatures R. A. SaravananJ. M. MolinaE. Louis OriginalPaper Pages: 309 - 311
Synthesis of strontium hexaboride powder by the reaction of strontium carbonate with boron carbide and carbon Shu-Qi ZhengZeng-Da ZouWei-Ti Wang OriginalPaper Pages: 313 - 315
Development of carbon-ceramic composites through sol-gel and particulate routes V. RamanG. BhatiaA. Mishra OriginalPaper Pages: 317 - 320
Growth of Fe4N thin films by atmospheric pressure vapor phase epitaxy N. TamuraN. TakahashiT. Takahashi OriginalPaper Pages: 321 - 323
Improvement of interface morphology between titanium-silicide and poly-Si thin film using Ar plasma treatment Jae-Moon ChoiDae-Jung KimMyoung-Gi So OriginalPaper Pages: 325 - 328
Microindentation testing of environmental stress cracked welds in polyethylene Y. LuD. M. ShinozakiS. Herbert OriginalPaper Pages: 329 - 332
Apple residue—new starting material for high surface area carbon B. Y. ZhaoT. HiroseD. Zhang OriginalPaper Pages: 333 - 336
Hybrid and conventional particle reinforced metal matrix composites by squeeze infiltration casting R. SahaE. MorrisS. M. Pickard OriginalPaper Pages: 337 - 339
Disperse structures of undercooled Co-40 wt% Cu droplets processed in drop tube C. D. CaoB. WeiD. M. Herlach OriginalPaper Pages: 341 - 343
Coordination and phase separation in polyvinylpyrrolidone-neodymium chloride complex Aifang XieZebo ZhangDuanfu Xu OriginalPaper Pages: 345 - 347
Development for silicon carbide fibers with trilobal cross section Yingde WangYanmo ChenYingchun He OriginalPaper Pages: 349 - 350