Correction to: Cellulose https://doi.org/10.1007/s10570-023-05708-5

In the original publication of the article, Figs. 7 and 8 were duplicated. The correct version of the Figs. 7 and 8 are provided in this correction.

Fig. 7
figure 7

Surface morphology of PALF as observed by SEM images: a 101.6 mm cut-length fourth carded (L4C); b 101.6 mm cut-length fifth carded (L5C); c 76.2 mm cut-length fourth carded (M4C); d 76.2 mm cut-length fifth carded (M5C); e 50.8 mm cut-length fourth carded (S4C); and f 50.8 mm cut-length fifth carded (S5C)

Fig. 8
figure 8

a X-ray diffraction pattern; b crystallinity (%) and cellulose (%) of PALF samples

The original article has been corrected.