Deformation and deformation-specific microstructures associated with a hypervelocity impact crater in copper S. A. QuinonesJ. M. RivasL. E. Murr OriginalPaper Pages: 685 - 688
Interband transitions of Al0.35Ga0.65As/GaAs multiple quantum wells Y. T. OhT. W. KangT. W. Kim OriginalPaper Pages: 689 - 691
Dielectric constant versus ageing time for the doped PMN-PZN-PT ferroelectric relaxor ceramic of Z5U MLCs Wang YuGui ZhilunZhang Xiaowen OriginalPaper Pages: 695 - 696
Anomalous temperature dependence of the sound velocities of SiO2-TiO2 glasses K. HiraoK. TanakaN. Soga OriginalPaper Pages: 697 - 699
The relationship between the defects of alpha-Si3N4 whiskers and growth temperature Ke-Hong ZhangGong-Hua XuHua-Wu Wu OriginalPaper Pages: 700 - 704
Mössbauer studies of R(Fe1−x Mn x )2 (R = Tb, Ho) intermetallic compounds Y. J. TangH. L. LuoS. M. Pan OriginalPaper Pages: 705 - 707
Modification of MgO surface for trace carbon analysis B. I. LeeT. E. DixonT. Sessions OriginalPaper Pages: 708 - 709
OH-related capacitance-voltage recovery effect in MOS capacitors passivated by PbO-B2O3-SiO2-MgO glasses VII, the effects of MgO content K. Kobayashi OriginalPaper Pages: 710 - 712
Fourier transformation infrared investigation of surface oxidation of ultrafine Si3N4 powders Y. -L. LiY. LiangT. Shun OriginalPaper Pages: 713 - 715
Effect of n-type semiconducting CdS substitution on the electrical properties and structure of Y-Ba-Cu-O oxide superconductors S. BanerjeeS. Chatterjee OriginalPaper Pages: 716 - 719
Microhardness studies on zinc doped cadmium sulphide single crystals K. BalakrishnanJ. KumarG. Attolini OriginalPaper Pages: 720 - 722
Slow crack growth in MgAl2O4 single- and poly-crystals R. W. RiceC. C M. Wu OriginalPaper Pages: 723 - 727
Synthesis and chemical stability of NaSn2P3O12 E. BrevalG. HarshéS. Y. Limaye OriginalPaper Pages: 728 - 731
Some peculiarities of the phase separation in the TeO2-B2O3-SiO2 system E. KashchievaY. Dimitriev OriginalPaper Pages: 732 - 735
Effect of grain size on scratch damage and hardness of alumina H. H. K. XuS. Jahanmir OriginalPaper Pages: 736 - 739
Effect of break-in speed on early stage sliding behaviour of two-dimensional PAN-pitch based carbon-carbon composite C. P. JuJ. D. ChenJ. H. Chern Lin OriginalPaper Pages: 740 - 743
Hydroxyapatite sintering characteristics: correlation with powder morphology bv high-resolution microscopy A. J. BuysC. C. SorrellB. K. Milthorpe OriginalPaper Pages: 744 - 747
Influence of sintering time on (Ba, Bi, Nb)-added TiO2 ceramic varistor S. -L. YangJ. -M. Wu OriginalPaper Pages: 748 - 751
Titanium solubility in the Fe-Zn intermetallic compounds when galvanizing iron substrates in Zn-Ti baths at 450 °C G. ReumontT. GloriantP. Perrot OriginalPaper Pages: 752 - 754
Degradation of SiC (Tyranno) fibres in high-temperature, high-pressure water Y. GogotsiM. Yoshimura OriginalPaper Pages: 755 - 759