The main forms and geometric parameters of chipping during diamond surface grinding are determined on the basis of studying features of the formation Y–TZP-ceramic edge morphology. A correlation is revealed between grinding depth, longitudinal and transverse feed with chipping geometric parameters.
Similar content being viewed by others
References
V. V. Kuzin, S. Yu. Fedorov, and S. N. Grigor’ev, “Correlation of diamond grinding regime with surface condition of ceramic based on zirconium dioxide,” Refract. Indust. Ceram., 57(6), 625 – 630 (2017).
V. V. Kuzin, S. Yu. Fedorov, and S. N. Grigor’ev, “Features of specimen edge morphology formation for Al2O3–TiC ceramic with diamond grinding,” Novye Ogneupory, No. 5, 63 – 67 (2017).
This work is supported by The Russian Federation Ministry of Education and Science within the scope of a state assignment of MGTU STANKIN in the sphere of scientific activity (assignment 9.1372.2017/4.6).
Author information
Authors and Affiliations
Corresponding author
Additional information
Translated from Novye Ogneupory, No. 7, pp. 63 – 65, July, 2017.
Rights and permissions
About this article
Cite this article
Kuzin, V.V., Fedorov, S.Y. & Grigor’ev, S.N. Level of Y–TZP-Ceramic Specimen Edge Defects After Diamond Machining. Refract Ind Ceram 58, 415–417 (2017). https://doi.org/10.1007/s11148-017-0121-0
Received:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s11148-017-0121-0