Abstract
The results of an investigation of the porous structure of the Al2O3-SnO2 system and its properties after hydrogen treatment are presented. Pore size distribution was determined on the basis of low temperature nitrogen adsorption measurements. Reduction of the system by H2 leads to a decrease of the parameters defining porous structure. We conclude that this is due to the reduction of Sn(IV) species to oxidation state II.
Similar content being viewed by others
References
E.W. Thornton and P.G. Harrison, J. Chem. Soc. Faraday Trans. 171 (1975) 461.
K. Weters and C. Misra, in:Oxides and Hydroxides of Aluminum, Alcoa Technical Paper No. 19 (Alcoa, 1987).
G.D. Chookin and I.L. Seleznev, Kinet. Catal. 30 (1989) 69.
J.S. Wilson, J. Solid State Chem. 30 (1979) 247.
P. Burtin, J.P. Brunelle, M. Pijolat and M. Soustelle, Appl. Catal. 34 (1987) 225.
V.I. Vereshchagin, V.Yu. Zelinski, T.A. Khabas and N.N. Kolove, Zh. Prikl. Khim. 55 (1982) 1946.
S. Janiak and J. Wrzyszcz,Preparation of Catalysts (Elsevier, Amsterdam, 1976) p. 663.
H. Krischner, K. Tokar and P. Hornisch, Monatsh. Chem. 99 (1968) 330.
P. Kirszensztejn, Mater. Chem. Phys. 27 (1991) 117.
S. Matsuda, S. Koto, M. Mizumoto and H. Yamashita,8th Int. Congr. on Catalysis, Vol. 4, Berlin (1984) p. 879.
J.M. Schwaller, P. Wehrer, F. Garin and G. Maive, Ann. Chim. Fr. 14 (1989) 208.
G.C. Bye and G.T. Simpkin, J. Am. Ceram. Soc. 57 (1974) 367.
P. Kirszensztejn, W. Przystajko and T.N. Bell, Catal. Lett. 18 (1993) 391.
P. Kirszensztejn, Z. Foltynowicz, S. Zielinski and G.B. Hoflund, Ann. Chim Fr. 14 (1989) 449.
P. Kirszensztejn, Mater. Chem. Phys. 27 (1991) 129.
P. Kirszensztejn, Z. Foltynowicz and L. Wachowski, Ind. Eng. Chem. Res. 30 (1991) 2277.
P. Kirszensztejn and S. Zielinski, Polish Patent PL-275654(1988).
R.W. Cranston and F.A. Inkley, Adv. Catal. 9 (1957) 143.
T.C. Sheng, P. Kirszensztejn, T.N. Bell and I.D. Gay, Catal. Lett., in press.
P.G. Harrison, in:Chemistry of Tin (Chapman and Hall, New York, 1989).
K.S.W. Sing, D.H. Everet, R.A.W. Haul, L. Moscou, R.A. Pierotti, J. Rouquerol and T. Siemieniewska, Pure Appl. Chem. 57 (1985) 606.
S. Soled, J. Catal. 81 (1983) 252.
M.J. Fuller and M.E. Warwick, J. Catal. 29 (1973) 441.
G. Croft and M.J. Fuller, Nature 269 (1977) 585.
M. Ai, J. Catal. 40 (1975) 318, 327.
B.M. Mounders, PhD Thesis, University of Nottingham, UK(1982).
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Kirszensztejn, P., Bell, T.N. Effect of hydrogen treatment on the porous structure of Al2O3-SnO2 system. Catal Lett 21, 371–380 (1993). https://doi.org/10.1007/BF00769489
Received:
Accepted:
Issue Date:
DOI: https://doi.org/10.1007/BF00769489