Abstract
A new method has been developed for the corrosion protection of steel parts: gas-phase coating application. The resulting coating is characterized by high density, chemical resistance to aggressive media, and good surface adhesion. This method may be used for parts of complex shape. The static and fatigue failure of БСт.3сп, 40, and Э10 steel is investigated, in the presence of nickel coatings of different thickness, applied at different temperatures.
Similar content being viewed by others
REFERENCES
Pachurin, G.V. and Pachurin, K.G., Fatigue destruction of metals and alloys, Tekhnol. Met., 2005, no. 5, pp. 7–11.
Pachurin, G.V., Service life of plastically threatened steels and welded joints, Kuznechno-Shtampovochnoe Proizvod.–Obrab. Mater. Davleniem, 2004, no. 12, pp. 3–8.
Pachurin, G.V., Pachurin, K.G., and Vlasov, V.A., Selection of forging equipment, Tyazh. Mashinostr., 2005, no. 10, pp. 38–40.
Filippov, A.A., Pachurin, G.V., Naumov, V.I., and Kuz’min, N.A., Low-cost treatment of rolled products used to make long high-strength bolts, Metallurgist, 2016, vol. 59, nos. 9–10, pp. 810–815.
Filippov, A.A., Pachurin, G.V., Matveev, Yu.I., et al., Comparison of preparation methods of the structural and mechanical properties of the rolling surface for the upsetting of metal goods to reduce the impact on workers of hazardous and harmful factors, Fundam. Issled., 2016, no. 10-1, pp. 88–96.
Filippov, A.A., Pachurin, G.V., and Kuz’min, N.A., Reduction of hazardous and harmful factors during purification of the surface of rolled steels, Sovrem. Naukoemkie Tekhnol., 2016, no. 2-1, pp. 38–43.
Pachurin, G.V. and Vlasov, V.A., Mechanical properties of sheet structural steels at operating temperatures, Met. Sci. Heat Treat., 2014, vol. 56, nos. 3–4, pp. 219–223.
Pachurin, G.V., Durability of forged construction materials in air and in corrosive environment, Zagotovitel’nye Proizvod. Mashinostr., 2003, no. 10, pp. 21–27.
Pachurin, G.V., Durability of deformed steels in air and in corrosive environment, Tekhnol. Met., 2004, no. 12, pp. 29–35.
Pachurin, G.V., Ruggedness of structural material and working life of metal components, Steel Transl., 2008, vol. 38, no. 3, pp. 217–220.
Pachurin, G.V. and Guslyakova, G.P., Optimizatsiya rezhimov tekhnologicheskoi obrabotki s tsel’yu povysheniya soprotivleniya korrozionno-ustalostnomu razrusheniyu metallicheskikh materialov (Optimization of Technological Treatment Modes to Improve Resistance to Corrosion-Fatigue Destruction of Metal Materials), Nizhny Novgorod: Mashprom, 1991.
Novikov, I.I., Defekty kristallicheskogo stroeniya metallov (Defects of Crystalline Structure of Metals), Moscow: Metallurgiya, 1983.
Sokolov, L.D. and Guslyakova, G.P., The identification of thermally activated mechanisms controlling the fatigue, Izv. Akad. Nauk SSSR, Met., 1979, no. 4, pp. 141–145.
Karpenko, G.V., Pokhmurskii, V.I., Dalisov, V.B., and Zamikhovskii, V.S., Vliyanie diffuzionnykh pokrytii na prochnost’ stal’nykh izdelii (Effect of Diffusive Coatings on the Strength of Steel Products), Kiev: Naukova Dumka, 1971.
Author information
Authors and Affiliations
Corresponding author
Additional information
Translated by Bernard Gilbert
About this article
Cite this article
Pachurin, G.V., Kuz’min, N.A., Filippov, A.A. et al. Mechanical Properties of Steel after Gas-Phase Application of a Nickel Coating. Russ. Engin. Res. 39, 577–579 (2019). https://doi.org/10.3103/S1068798X19070153
Received:
Revised:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.3103/S1068798X19070153