Abstract
Laboratory data indicate the positive effects of introducing fluorocarbon and nickel in 25Kh5FMS steel powder wire for the surfacing of rollers. In particular, the replacement of amorphous carbon by a material containing fluorocarbon lowers the content of nonmetallic inclusions in the applied layer, while introducing nickel in the powder wire reduces the austenite grain size and ensures the formation of small carbide particles. That increases the thermal stability of the applied layer. Increase in the carbon equivalent of the 25Kh5FMS powder wire boosts the hardness of the applied metal layer.
Similar content being viewed by others
References
Danilov, L.I., Skorokhvatov, N.B., and Sobolev, V.F., Increase of service life period of counter rollers of 2000 rolling mill of hot strip rolling at JSC Severstal, Chern. Metall., 2004, no. 8, pp. 68, 69.
Ogarkov, N.N. and Belyaev, A.I., Stoikost’ i kachestvo prokatnykh valkov (Durability and quality of rolls), Magnitogorsk: Magnitogorsk. Gos. Tekh. Univ., 2008.
Matvienko, V.N., Gulakov, S.V., and Royanov, V.A., Reduction with welding of the parts of metallurgical equipment in the conditions of Ilyich Iron and Steel Works, Met. Lit’e Ukr., 2005, nos. 7–8, pp. 66–69.
Gulidov, I.N., Oborudovanie prokatnykh tsekhov: ekspluatatsiya i nadezhnost’ (Equipment of Rolling-Mill Shops: Service and Durability), Moscow: Intermet Inzhiniring, 2004.
Traino, A.I., Rational roller operation and restoration, Steel Transl., 2008, vol. 38, no. 10, pp. 871–875.
Shebanits, E.N., Omel’yanenko, N.I., Kurakin, Yu.N., Matvienko, V.N., Leshchinskii, L.K., Dubinskii, B.E., and Stepnov, K.K., Improving the fracture toughness and wear resistance of hard-faced hot-rolling-mill rolls, Metallurgist, 2012, vols. 613–617, nos. 7–8, pp. 613–617.
Ryabtsev, I.A. and Kondrat’ev, I.A., Mekhanizirovannaya elektrodugovaya naplavka detalei metallurgicheskogo oborudovaniya (Mechanical Electric-Arc Welding of the Parts of Metallurgical Equipment), Kiev: Ekotekhnologiya, 1999.
Kal’yanov, V.N. and Novitskaya, A.V., Increase of durability of rolling mills when welding with economically alloyed steel, Svar. Proizvod., 1997, no. 10, pp. 23–27.
Kondrat’ev, I.A., Ryabtsev, I.A., and Kuskov, Yu.M., Arc and electroslag hard-facing of rollers of rolling mills, Svarshchik, 2004, no. 1, pp. 7–9.
Titarenko, V.I., Golyakevich, A.A., Orlov, L.N., Mosypan, V.V., Babenko, M.A., Telyuk, D.V., and Tarasenko, V.V., Reducing welding of rollers of rolling mills with powder cored wire, Svar. Proizvod., 2013, no. 7, pp. 29–32.
Kozyrev, N.A., Kryukov, R.E., Roor, A.V., Bashchenko, L.P., and Lipatova, U.I., New carbon-fluorine additives for welding fluxes, Steel Transl., 2015, vol. 45, no. 4, pp. 251–253.
Kozyrev, N.A., Titov, D.A., Starovatskaya, S.N., Kozyreva, O.E., and Shurupov, V.M., Influence of the addition of wire of C–Si–Mn–Cr–V–Mo carboncontaining additive and nickel, Izv. Vyssh. Uchebn. Zaved., Chern. Metall., 2014, no. 4, pp. 34–37.
Kozyrev, N.A., Kryukov, N.E., Kryukov, R.E., Igushev, V.F., and Koval’skii, I.N., Technological aspects of using a carbon–fluorine-containing addition in submerged- arc welding, Weld. Int., 2016, vol. 30, no. 4, pp. 325–328.
Makarov, E.L. and Yakushin, B.F., Teoriya svarivaemosti stalei i splavov (Theory of Welding Characteristics of Steels and Alloys), Moscow: Mosk. Gos. Tekh. Univ. im. N.E. Baumana, 2014.
Lakhtin, Yu.M. and Leont’eva, V.P., Materialovedenie (Material Science), Moscow: Al’yans, 2013.
Author information
Authors and Affiliations
Corresponding author
Additional information
Original Russian Text © N.A. Kozyrev, N.V. Kibko, A.A. Umanskii, D.A. Titov, A.G. Nikitin, 2016, published in Izvestiya Vysshikh Uchebnykh Zavedenii, Chernaya Metallurgiya, 2016, No. 10, pp. 727–734.
About this article
Cite this article
Kozyrev, N.A., Kibko, N.V., Umanskii, A.A. et al. New C–Si–Mn–Cr–V–Mo powder wires for roller surfacing. Steel Transl. 46, 711–717 (2016). https://doi.org/10.3103/S0967091216100053
Received:
Published:
Issue Date:
DOI: https://doi.org/10.3103/S0967091216100053