The quality of corrosion-resistant steel pipe is critical to energy conservation. Prospective requirements on such pipe call for a fundamental change in the manufacturing technology, including higher internal-surface quality, limited residual stress, and minimum chloride ions at the surface.
Similar content being viewed by others
References
Janikovski, D.S., Plymouth Tube, Heat Exchanger Maintenance and Retubing: Can You Afford to Wait? Tube Pipe Technol., 2007, vol. 20, no. 6, pp. 138–143.
Hones, C. and Harrison, A., Importance of Surface Finish in the Design of Stainless Steel, Stainless Steel Ind., 2006, no. 8, pp. 14–15.
Kuznetsov, D.E., Improving the Dimensional Precision and Surface Quality of Cold-Rolled Pipe, Stal’, 2005, no. 10, pp. 81–84.
Banyuk, G.F., Arkhipov, O.P., Brykov, S.I., et al., Development of Ongoing Monitoring of Steam-Generator Corrosion, Materialy 7-go mezhdunarodnogo seminara po gorizontyal’nym parogeneratoram (Proceedings of Seventh International Seminar on Horizontal Steam Generators), Podol’sk: FGUP Gidropress, 2006, pp. 1–7.
Kuznetsov, D.E., Vakhrusheva, V.S., and Kuznetsov, E.D., Interchangeability of Fuel-Rod Casings in Atomic Reactors, Vopr. atomnoi nauki i tekhniki: ser. Fizika radiatsionnykh povrezhdenii i radiatsionnoe materialovedenie (Atomic Science and Engineering: Physics of Radiation Damage and Radiative Materials Science), Khar’kov: NNTs Khar’kovskii Fiziko-Tekhnicheskii Institut, 2006, no. 4, pp. 47–55.
Author information
Authors and Affiliations
Additional information
Original Russian Text © E.D. Kuznetsov, E.E. Chigirinets, 2010, published in “Stal’,” 2010, No. 2, pp. 48–51.
About this article
Cite this article
Kuznetsov, E.D., Chigirinets, E.E. Improving the manufacture of corrosion-resistant steel pipe for power plants. Steel Transl. 40, 160–163 (2010). https://doi.org/10.3103/S0967091210020142
Published:
Issue Date:
DOI: https://doi.org/10.3103/S0967091210020142