Abstract
We have investigated the processes of pyroxene formation in crystallization of glasses of the system SiO2–Al2O3–CaO–MgO–Na2O stimulated with chromium and iron oxides introduced together. It is found that sharp activation of the processes of pyroxene formation occurs in the temperature interval of thermal treatment 850–900°C. Interpretation of the absorption bands is carried out and conclusions are drawn on the structural role of the iron and aluminum ions in the process of formation of a pyroxene solid solution.
Similar content being viewed by others
REFERENCES
L. A. Zhunina, M. I. Kuz'menkov, and V. N. Yaglov, in: Pyroxene Sitalls [in Russian], Minsk (1974), pp. 56–100, 153-212.
I. I. Plyusnina, in: Infrared Spectra of Silicates [in Russian], Moscow (1967), pp. 58–67.
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Bobkova, N.M., Barantseva, S.E. Effect of Fe2O3 and Cr2O3 on the Processes of Pyroxene Formation in Silicate Glasses. Journal of Applied Spectroscopy 69, 675–678 (2002). https://doi.org/10.1023/A:1021540525668
Issue Date:
DOI: https://doi.org/10.1023/A:1021540525668