Abstract

The effects of boron content (CB = 0–0.14% (mass fraction)) on the tensile properties and environmental embrittlement of ordered Ni-24%Fe (atom fraction)-B (Ni3Fe-B) alloys have been investigated using tensile tests in vacuum and under gaseous hydrogen. The results indicate that, when CB < 0.06% (mass fraction), the tensile strength and elongation of the alloys in vacuum and gaseous hydrogen increase as CB in the ordered Ni3Fe-B alloy increases. The tensile strength and elongation are maximum, and the hydrogen embrittlement factor (IH) is minimum for the ordered Ni3Fe-0.06%B (mass fraction) alloy. Compared with the ordered B-free Ni3Fe alloy, IH of the ordered Ni3Fe-0.06%B (mass fraction) alloy decreases by 98.1%, and the fracture morphology of the alloy changes from fully intergranular to fully transgranular, when tested in gaseous hydrogen. A critical level of boron segregation at the grain boundaries of ordered Ni3Fe-B alloys is observed. The hydrogen embrittlement of ordered Ni3Fe-B alloys in gaseous hydrogen can be completely suppressed by boron atoms when CB \(\geqslant\) 0.06% (mass fraction).

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Fig.1
Fig.2
Fig.3
Fig.4
Fig.5
Fig.6

Similar content being viewed by others

References

  1. Tao ZX (1990) Main properties and toughening methods of high technology structural materials for intermetallic compounds. Shanghai Steel Iron Res 6:51–58

    Google Scholar 

  2. Stoloff NS, Liu CT, Deevi SC (2000) Emerging applications of intermetallics. Intermetallics 8:1313–1320

    Article  Google Scholar 

  3. Wan XJ, Chen YX, Cheng XY (2001) Advances in research on environmental hydrogen embrittlement of intermetallic compounds. Prog Nat Sci 11(5):458–464

    Google Scholar 

  4. Wan XJ, Cheng XY, Chen YX et al (2001) Embrittlement of intermetallics in gaseous hydrogen. Prog Nat Sci 11(12):1233–1239

    Google Scholar 

  5. Camus GM, Stoloff NS, Duquette DJ (1989) The effect of ordering on the hydrogen embrittlement of Ni3Fe. Acta Metall 37(5):1497–1501

    Article  Google Scholar 

  6. Aoki A, Izumi O (1979) Improvement in room temperature ductility of the L12 type intermetallic Ni3Al by boron addition. Nippon Kinzoku Grakkaishi 43:1190–1199

    Google Scholar 

  7. Ma J, Chen YX, Liu CT (2009) Effect of boron on the environmental embrittlement of ordered Ni3Fe alloys in gaseous hydrogen. J Nanjing Univ 45(2):241–247

    Google Scholar 

  8. Wan XJ, Chen YX, Shi DD et al (2008) Effect of alloy stoichiometry and boron doping on the H2-induced environmental embrittlement of Ni3Fe intermetallics. Intermetallics 16:550–553

    Article  Google Scholar 

  9. Chen YX, Ma J (2012) Mechanism of boron suppressing environmental embrittlement in H2 for the ordered Ni3Fe intermetallics. Procedia Eng 27:1121–1128

    Article  Google Scholar 

  10. Liu Y, Liu CT, Heatherly L et al (2011) Effect of boron on the fracture behavior and grain boundary chemistry of Ni3Fe. Scr Mater 64(3):303–306

    Article  Google Scholar 

  11. Chen YX (2011) Environmental hydrogen embrittlement of intermetallics. J Shanghai Univ (Nat Sci) 17(4):487–502

    Google Scholar 

  12. Ma J (2008) Effect of boron on the environmental embrittlement of ordered Ni3Fe alloys in gaseous hydrogen. Dissertation, Shanghai University

  13. Takasugi T, Hanada S (1994) The influence of constituent elements and atomic ordering on hydrogen embrittlement of Ni3Fe polycrystals. Intermetallics 2:225–232

    Article  Google Scholar 

  14. Lee KH, Lukowski JT, White CL (1997) Effects of gaseous hydrogen and water vapor pressure on environmental embrittlement of Ni3Al. Intermetallics 5:483–490

    Article  Google Scholar 

  15. Wan XJ, Zhu JH, Jing KL (1992) Hydrogen effect on the deformation and fracture behaviors of a Ni3Al+B alloy. Scr Metall Mater 26:479–484

    Article  Google Scholar 

  16. Li J, Xie YP, Chen YX et al (2014) First-principles study of the hydrogen adsorption and diffusion on ordered Ni3Fe(111) surface and in the bulk. Intermetallics 44:64–72

    Article  Google Scholar 

  17. Chen YX, Ma J, Liu CT (2011) Hydrogen diffusivity in B-doped and B-free ordered Ni3Fe alloys. Intermetallics 19:105–108

    Article  Google Scholar 

  18. Yang B, Chen YX, Li SL (2018) Effect of B content on environmental embrittlement of ordered (Fe, Co)3V alloys. Rare Metal Mater Eng 3:976–981

    Google Scholar 

  19. Wan XJ, Zhu JH, Jing KL (1992) Environmental embrittlement in Ni3Al+B. Scr Metall Mater 26:473–477

    Article  Google Scholar 

Download references

Author information

Authors and Affiliations

Authors

Corresponding author

Correspondence to Ye-Xin Chen.

Rights and permissions

Reprints and permissions

About this article

Check for updates. Verify currency and authenticity via CrossMark

Cite this article

Chen, T., Chen, YX., Yang, B. et al. Effects of boron content on environmental embrittlement of ordered Ni3Fe alloys. Adv. Manuf. 7, 221–227 (2019). https://doi.org/10.1007/s40436-019-00255-4

Download citation

  • Received:

  • Accepted:

  • Published:

  • Issue Date:

  • DOI: https://doi.org/10.1007/s40436-019-00255-4

Keywords

Navigation