Abstract
The development of coating materials and processes was carried out with the objective to reduce material degradation in supercritical water. Based on the test results of bulk coating alloys (FeCrAlY and NiCrAl), two coating processes, plasma spray of dense NiCrAlY and pack aluminizing, have been developed to apply coatings to candidate stainless steels and Ni-based alloys. The SCW test results and microstructure characterization of both coating alloys and coated candidate alloys are presented in this short paper.
Similar content being viewed by others
References
A Technology Roadmap for Generation IV Nuclear Energy System (GIF 002-00, 2002), https://www.gen-4.org/gif/jcms/c_40473/a-technology-roadmap-for-generation-iv-nuclear-energy-systems. Accessed 12 Dec 2015.
Supercritical Water Reactor-Survey of Materials Experience and R&D Needs to Assess Viability (INEEL/EXT-03-00693, 2003), https://inldigitallibrary.inl.gov/sti/2699863.pdf. Accessed 12 Dec 2015.
G.S. Was, P. Ampornrat, G. Gupta, S. Teysseyre, E.A. West, T.R. Allen, K. Sridharan, L. Tan, Y. Chen, X. Ren, and C. Pister, J. Nucl. Mater. 371, 176 (2007).
J. Kaneda, S. Kasahara, F. Kano, N. Saito, T. Shikama, and H. Matsui, 5th Int. Sym. SCWR (ISSCWR-5), Vancouver, Canada, March 13–16, 2011.
L. Tan, M.T. Machut, K. Sridharan, and T.R. Allen, Transactions of the 2006 ANS Annual Meeting, Reno, NV, 94, 745 (2006)
S. Teysseyre, S. Jiao, E. West, and G.S. Was, J. Nucl. Mater. 371, 107 (2007).
P. Kritzer, J. Supercrit. Fluids 29, 1 (2004).
Q.J. Peng, S. Teysseyre, P.L. Andresen, and G.S. Was, Corrosion 63, 1033 (2007).
Y. Yi, B. Lee, S. Kim, and J. Jang, Mater. Sci. Eng., A 429, 161 (2006).
L.R. Greenwood, J. Nucl. Mater. 115, 137 (1983).
S. Teysseyre and G.S. Was, Corrosion 62, 1100 (2006).
A. Aguero, R. Muelas, and V. Gonzalez, Mater. Corros. 59, 393 (2008).
A. Qian, X. Huang, and D. Guzonas, 5th Int. Sym. SCWR (ISSCWR-5), Vancouver, Canada, March 13–16, 2011.
S. Biljan, A. Qian, X. Huang, and D. Guzonas, 5th Int. Sym. SCWR (ISSCWR-5), Vancouver, Canada, March 13–16, 2011.
X. Huang, D. Guzonas, and J. Li, Corros. Eng. Sci. Tech. 50, 137 (2015).
X. Huang and D. Guzonas, J. Nucl. Mater. 445, 298 (2014).
P. Xu, L. Zhao, K. Sridharan, and T. Allen, J. Nucl. Mater. 422, 143 (2012).
J. Bischoff, A. Motta, C. Eichfeld, R. Comstock, G. Cao, and T. Allen, J. Nucl. Mater. 441, 604 (2013).
T. Allen, K. Sridharan, Y. Chen, L. Tan, X. Ren, and A. Kruizenga, ICPWS XV, Berlin, Sept. 8–11, 2008.
S.H. Nie, Y. Chen, X. Ren, K. Sridharan, and T.R. Allen, J. Nucl. Mater. 399, 231 (2010).
S. Penttila, Materials for the SCWR Concept, GEN4FIN Seminar, Lappeenranta, Oct. 2–3, 2008.
Y. Qian, X. Huang, and D. Guzonas, The 3rd China-Canada Joint Workshop on Supercritical Water-Cooled Reactors (CCSC-2012), Shenzhen, China, April 18–20, 2012.
A. Selvig, X. Huang, D.-J. Kim, and Dave Guzonas, J. Mater. Corros. (2012). doi:10.1002/maco.201206613.
X. Huang, Q. Yang, and D. Guzonas, J. Nucl. Rad. Sci., in press, 2015. doi:10.1115/1.4031198.
F. Barrett, X. Huang, and D. Guzonas, J. Therm. Spray Technol. 22, 734 (2013).
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Huang, X. Developing Corrosion Prevention Coating Solutions for the Canadian SCWR Concept. JOM 68, 480–484 (2016). https://doi.org/10.1007/s11837-015-1742-8
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s11837-015-1742-8