Abstract
Dynamic mechanical and thermal properties of poly(ester urethanes) (PEU) cross-linked with styrene have been studied. The investigated polyurethanes were obtained from 4,4′-diphenylmethane diisocyanate and unsaturated oligo(alkyleneester)diol based on cis-2-butene-1,4-diol. The conducted analyses dealt with the correlation between the chemical structure of poly(ester urethanes) and their ability to phase separate as well as their thermal stability. The products of PEU thermal degradation were characterized using infrared spectroscopy.
Similar content being viewed by others
References
G. Oertel, Polyurethane Handbook, Hanser Publishers, New York 1985.
D. Randall and S. Lee, The Polyurethanes Book, John Wiley and Sons 2002.
R. J. Lin and L. W. Chen, J. Appl. Polym. Sci., 73 (1999) 1305.
M. Spirkova, L. Matejka, D. Hlavata, B. Meissner and J. Pytela, J. Appl. Polym. Sci., 77 (2000) 381.
R. Samborska-Skowron and A. Balas, Polym. Adv. Technol., 13 (2002) 653.
A. Koscielecka, Acta Polym., 42 (1991) 221.
H. Ni, J. L. Daum, P. R. Thiltgen, M. D. Soucek, W. J. Simonsick, W. Zhong and A. D. Skaja, Prog. Org. Coat., 45 (2002) 49.
B. Gawdzik, T. Matynia and J. Osypiuk, J. Appl. Polym. Sci., 79 (2001) 201
Ph. Radenkov, M. Radenkov, G. Grancharov and K. Troev, Eur. Polym. J., 39 (2003) 1223.
V. Sekkar, K. N. Ninan, V. N. Krishnamurthy and S. R. Jain, Eur. Polym. J., 36 (2000) 2437.
T. Gupta and B. Adhikari, Thermochim. Acta, 402 (2003) 169.
F. M. B. Cautinho, M. C. Delpech, T. L. Alves and A. A. Ferreira, Polym. Degrad. Stab., 81 (2003) 19.
V. Thomas and M. Jayabalan, Biomaterials, 23 (2002) 273.
S. Sarkar and B. Adhikari, Polym. Degrad. Stab., 73 (2001) 169.
D. J. Harris, R. A. Assink and M. Celina, Macromolecules, 34 (2001) 6695.
V. Sekkar, S. S. Bhagawan, N. Prabhakaran, M. R. Rao, and K. N. Ninan, Polymer, 41 (2000) 6773.
A. Balas, G. Pałka, B. Płomińska and M. Rutkowska, Acta Polym., 31 (1980) 673.
S. H. O. Egboh, J. Macromol. Sci. Chem., A(19) (1983) 1041.
L. Jasińska, A. Balas and J. T. Haponiuk, e-Polymers, 003 (2007).
L. Jasińska, A. Balas, J. T. Haponiuk, G. Nowaczyk and S. Jurga, J. Therm. Anal. Cal., 88 (2007) 419.
M. Herrera, G. Matuschek and A. Kettrup, Polym. Degrad. Stab., 78 (2002) 323.
K. Pielichowski and A. Leszczyńska, J. Therm. Anal. Cal., 78 (2004) 631.
K. Nakamura, Y. Nishimura, P. Zetterlund, T. Hatakeyama and H. Hatakeyama, Thermochim. Acta, 282 (1996) 433.
J. Datta and M. Rohn, J. Therm. Anal. Cal., 88 (2007) 437.
P. S. Wang, W. Y. Chiu, L. W. Chen, B. L. Deng, T. M. Don and Y. S. Chiu, Polym. Degrad. Stab., 66 (1999) 307.
M. Bautin, J. Lesage, C. Ostiguy, J. Pauluhn and M. J. Bertrand, J. Anal. Appl. Pyrolysis, 71 (2004) 791.
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Jasińska, L., Haponiuk, J.T. & Balas, A. Dynamic mechanical properties and thermal degradation process of the compositions obtainedfrom unsaturated poly(ester urethanes) cross-linked with styrene. J Therm Anal Calorim 93, 777–781 (2008). https://doi.org/10.1007/s10973-008-9201-1
Published:
Issue Date:
DOI: https://doi.org/10.1007/s10973-008-9201-1