Abstract
Multiblock terpolymer of poly(L-lactic acid)/ poly(ethylene oxide)/poly(L-aspartic acid), (PLLA/PEO/ PAsp) was synthesized by ring opening polymerization of β -benzyl L-aspartate N-carboxyanhydride, Asp(OBzl)-NCA with α-ω -hydroxy terminated triblock PLLA/PEO/PLLA copolymer.
The resulting multiblock terpolymer was characterized by several techniques including Fourier transform infrared spectroscopy and differential scanning calorimetry.1H nuclear magnetic resonance spectra indicated the molar ratio of PLLA/PEO/PAsp (OBzl) to be 86/10/4.
Thermal gravimetric analysis and environmental scanning electron microscopy data showed that PLLA/PEO/PAsp had crystalline and brittle structure. In order to improve its mechanical and physical properties, the terpolymer was blended with high molecular weight poly(L-lactic-co-glycolic acid) copolymer, PLGA(85/15) (Mw: 95000 gmol− 1) in 25/75 and 50/50 mole ratios.
The hydrolytical degradation properties of these polymers were studied. Degradation experiments were performed during a 48-day period in pH:7.4 phosphate-buffered saline (PBS) at 37∘C. The observed molecular weight losses were 91% and 67% for the 25/75 and 50/50 mixtures, respectively. In vitro attachment and growth of L929 mouse fibroblasts on these biopolymers were also investigated. Cell growth experiments indicated that the copolymer blend allowed the attachment and growth of cells.
Similar content being viewed by others
References
D. K. GILDING and A. M. REED, Polymer, 20 (1979), 1459.
F. E. KOHN, J. W. A. VAN DEN BERG, G. V. RIDDER, J. Appl. Polym. Sci. 29, 1984, 4265.
D. J. MOONEY, G. ORGAN, J. P. VACANTI and R. LANGER, Cell Transplant. 3, 1994, 203.
B. S. KIM and D. J. MOONEY, Trends Biotechnol. 16, 1998, 224.
D. J. MOONEY, S. PARK, P. M. KAUFMANN, K. SANO, K. MCNAMARA, J. P. VACANTI, R. LANGER, J. Biomed. Mater. Res. 29, 1995, 959.
P. J. A. VELD, Z. R. SHEN, G. A. J. TAKENS, P. J. DIJKSTRA and J. FEIJEN, J. Polym. Sci. Part A: Polym. Chem. 32, 1994, 1063.
D. A. BARRERA, E. ZYLSTRA, P. T. LANSBURY, R. LANGER, Macromolecules 28, 1995, 425.
J. S. HRKACH, J. OU, N. LOTAN, R. LANGER, Macromolecules 28, 1995, 4736.
G. JOHN, S. TSUDA, M. MORITA, J. Polym. Sci. Part A: Polym. Chem. 35, 1997, 1901.
T. OUCHI, T. NOZAKI, A. ISHIKAWA, I. FUJIMOTO and Y. OHYA, J. Polym. Sci. Part A: Polym. Chem. 35, 1997, 377.
E. B. LAVIK, J. S. HRKACH, N. LOTAN, R. NAZAROV and R. LANGER, J. Biomed. Mater. Res. 58, 2001, 291.
S. JO, P. S. ENGEL and A. G. MIKOS, Polymer 41, 2000, 7595.
H. SHINODA, Y. ASOU, A. SUETSUGU and K. TANAKA, Macromolecular Bioscience. 3, 2003, 34.
W. H. DALY and D. POCHE, Tetrahedron Letters 29, 1988, 5859.
J. S. HRKACH, J. OU, N. LOTAN and R. LANGER, Mat. Res. Soc. Symp. Proc. 394, 1995, 77.
J. S. HRKACH, J. OU, N. LOTAN and R. LANGER, ACS Symposium Series 627, 1996, 93.
N. KAYAMAN, O. KARAL-YILMAZ, K. BAYSAL and B. M. BAYSAL, Polymer 42, 2001, 4109.
Y. GUO, K. BAYSAL, B. KANG, L. J. YANG and J. R. WILLIAMSON, J. Biol. Chem. 273, 1998, 4027.
A. F. THUNEMANN, J. BEYERMANN and H. KUKULA, Macromolecules 33, 2000, 5906.
L. LU, S. J. PETER, M. D. LYMAN, H. L. LAI, S. M. LEITE, J. A. TAMADA, S. UYAMA, J. P. VACANTI, R. LANGER and A. G. MIKOS, Biomaterials. 21, 2000, 1837.
K. CAI, K. YAO, X. HOU, Y. WANG, Y. HOU, Z. YANG, X. LI and H. XIE, J. Biomed Mater Res. 62, 2002, 283.
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Karal-Yilmaz, O., Kayaman-Apohan, N., Misirli, Z. et al. Synthesis and characterization of poly(L-lactic acid-co-ethylene oxide-co-aspartic acid) and its interaction with cells. J Mater Sci: Mater Med 17, 213–227 (2006). https://doi.org/10.1007/s10856-006-7307-1
Received:
Accepted:
Issue Date:
DOI: https://doi.org/10.1007/s10856-006-7307-1