Chitin and chitosan with degree of deacetylation (DD) 57, 85, 89, and 90% were obtained as 250-μm microparticles. Their behavior with shear flow in aqueous and acidic solutions was studied. It was found that chitosan microparticles with various DD converted into gels as a result of swelling in water. Chitosan hydrogel particles with DD >85% were destroyed in shear flow without destroying the chains. The macromolecules were ordered in the direction of the flow.
Similar content being viewed by others
References
K. G. Skryabin, G. A. Vikhoreva, and V. P. Varlamov (eds.), Chitin and Chitosan: Production, Properties and Application [in Russian], Nauka, Moscow, 2002, 368 pp.
T. A. Akopova, S. Z. Rogovina, et al., Vysokomol. Soedin., Ser. B, 32, No. 10, 735-738 (1991).
A. A. Kholmuminov, V. O. Kudyshkin, et al., Vysokomol. Soedin., Ser. A, 52, No. 9, 1612-1614 (2010).
E. N. Fedoseeva, L. A. Smirnova, and V. B. Fedoseev, Vestn. Nizhegorodsk. Univ., Ser. Khim., No. 4, 59-64 (2008).
Author information
Authors and Affiliations
Corresponding author
Additional information
Translated from Khimicheskie Volokna, No. 4, pp. 31-33, July—August, 2015.
Rights and permissions
About this article
Cite this article
Kodirkhonov, M.R. Flow Behavior of Chitosan Particles. Fibre Chem 47, 251–252 (2015). https://doi.org/10.1007/s10692-016-9674-9
Published:
Issue Date:
DOI: https://doi.org/10.1007/s10692-016-9674-9