Abstract
For efficient production of display and touch sensing components of modern tablets and mobile communication devices, the bending strength of ultrathin glass must be enhanced for efficient processing in roll-to-roll process. Laser peeling is an effective method for enhancing the strength by removing edge defects on glass using irradiating CO2 laser pulses on glass edges to peel off a thin layer containing edge defects. However, this process involves complicated interaction in various fields such as heat transfer, stress, fracture, and phase change, as well as possible material properties variations. Without carefully selection of the processing conditions, the process can lose of control easily. To guide the process design for optimizing the laser peeling process and prevent failure, the mechanism of this material removal process is investigated individually, including the heat transfer model for analyzing transient temperature variation in a substrate being peeled and thermal stress induced structure fracture. Subsequently, essential parametric studies are performed later to characterize the influence of individual processing parameters. It was found that the depth of the heat affective zone has a strong impact on the peeling performance and the simulation results agree with that from experimental observations. Finally, by means of fracture mechanics and using the strain energy release rate as the measure, this work successfully explains the observed features and provide engineering basis for possible future process improvements. The laser peeling process is also successfully modelled as a moving temperature source for simulating the crack propagation during peeling using the extended finite element method. It is believed that through this study, the fundamental mechanism of laser peeling can be clearly understood, which would be vital for conducting subsequent process optimization and related glass packaging applications.
Similar content being viewed by others
References
Abaqus 6.9, Extended Functionality (EF) Overview (2009) Abaqus 6.9-EF Update Webinar, Dassault Systems
Fluegel A, Earl DA, Varshneya AK, Seward TP (2008) Density and Thermal expansion calculation of silicate glass melts from 1000 & #xB0;C to 1400 & #xB0;C. Phys Chem Glasses Eur J Glass Sci Technol B 49:245–257
Allcock G, Dyer PE, Elliner G, Snelling HV (1995) Experimental observations and analysis of CO2 laser-induced microcracking of glass. J Appl Phys 78:7295–7303
Benzeggagh ML, Kenane M (1996) Measurement of mixed-mode delamination fracture toughness of unidirectional glass/epoxy composites with mixed-mode bending apparatus. Comp Sci Technol 56:439–449
Li CH, Huang CJ, Chen KT, Lin MC (2014) The enhanced thin glass with an ultra-high bending strength by a laser peeling technology. Proc. The 21st International Display Workshops (IDW’14), Niigata, Japan, Paper FLXp1-12
Carslaw HS, Jaeger JC (1959) Conduction of Heat in Solids, 2nd edn. Clarendon Press, Oxford
Chen J, Liu CT (2013) Technology Advances in Flexible Displays and Substrates. IEEE Access 1:150–158
Chiu TC, Lin HC (2009) Analysis of stress intensity factors for three-dimensional interface crack problems in electronic packages using the virtual crack closure technique. Int J Fracture 156:75–96
Chow WT, Atluri SN (1995) Finite element calculation of stress intensity factors for interfacial crack using virtual crack closure integral. Comput Mech 16:417–425
Rosenthal D, Schmember R (1938) Thermal study of arc welding. Welding J Supplement 208
Erdogan F, Sih GC (1963) On the crack extension in plates under plane loading and transverse shear. J Basic Eng 85:519–527
Garner S, Glaesemann S, Li X (2014) Ultra-slim flexible glass for roll-to-roll electronic device fabrication. Appl Phys A 116(2):402–407
Kanninen MF (1973) An augmented double cantilever beam model for studying crack propagation and arrest. Int J Fract 9:83–92
Krueger R (2004) Virtual crack closure technique: history, approach, and applications. Appl Mech Rev 57:109–143
Chen KS, Yang T-S, Hong R-C, Chiu T-C, Wen ACD, Li C-H, Huang C-J, Chen K-T, Lin M-C (2016) Thermo-mechanical analysis of laser peeling of ultrathin glass for removing edge flaws in web processing applications. In: Proc. Design, Testing, Integration, and Packaging of MEMS and MOEMS (DTIP 2016), Budapest, Hungary
Pais M, Yeralan S, Davis T, Kim NH (2012) An exact reanalysis algorithm using incremental cholesky factorization and its application to crack growth modeling. Int J Num Methods Eng 91:1358–1364
Hong RC (2016) Finite element fracture analyses in elastic structures and its applications with case studies. Master Thesis, Department of Mechanical Engineering, National Cheng-Kung University, Taiwan
Rooke DP, Cartwright DJ (1976) Compendium of Stress Intensity Factors. HMSO Ministry of Defence. Procurement Executive
Li X, Garner S (2014) Laser cutting of flexible glass. Proc. CLEO Applications and Technology 2014, San Jose. Paper Atu3L.1
Mohammadi S (2008) Extended Finite Element Method for Fracture Analysis of Structures. Blackwell Publishing
Chiu TC, Hua C-A, Wang C-H, Chen K-S, Yang T-S, Wen C-D, Li C-H, Lin M-C, Huang C-J, Chen K-T (2016) On the mechanics of laser peeling for ultra-thin glasses. Eng Fract Mech (to appear)
Ugural AC, Fenster SK (2003) Advanced Strength and Applied Elasticity, 4th edn. Prentice-Hall
Hsiao YC (1997) Finite element analysis of laser forming. MS thesis, Department of Mechanical Engineering, Massachusetts Institute of Technology, USA
Yang TS, Chen GD, Chen K-S et al (2015) Thermal Analysis of a Laser Peeling Technique for Removing Micro Edge Cracks of Ultrathin Glass Substrates for Web Processing. Proc. ASME IMECE 2015, Huston
Wang ZK, Zheng HY (2012) Investigation on CO2 laser irradiation inducing glass strip peeling for microchannel formation. Biomicrofluidics 6(1):012820-1–012820-12
Zheng HY, Lee T (2005) Studies of CO2 laser peeling of glass substrates. J Micromech Microeng 15(11):2093–2097
Acknowledgements
The first author gratefully acknowledges partial support of this work in this endeavor by the Ministry of Science and Technology of Taiwan through Grant No. MOST 105-2221-E-006-074-MY3, ITRI-NCKU research center, and Silicon Valley Foundation (USA) under Grant No. B104-K27.
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Chen, KS., Yang, TS., Hong, RC. et al. Thermo-mechanical analysis of laser peeling of ultrathin glass for removing edge flaws in web processing applications. Microsyst Technol 24, 397–409 (2018). https://doi.org/10.1007/s00542-017-3300-5
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s00542-017-3300-5