Summary
Poly(vinyl alcohol) (PVA) layers of different thicknesses were intercalated into stereocomplex films composed of poly(L-lactide) and poly(D-lactide). The immersion of composite films into boiling water selectively extracted the water-soluble PVA components, resulting in porous stereocomplex films. The hydrolytic properties of the porous films under alkaline conditions were then quantitatively analyzed. It was observed that the hydrolytic rates decreased with increasing pore sizes.
Similar content being viewed by others
References
Ikada Y, Shikinami Y, Hara Y, Tagawa M, Fukada E (1996) J Biomed Mater Res 30:553
Asahi T, Fukase H, Ichiki M, Kobayashi J, Fukada E (1990) Ferroelectrics 109 : 339
Ikada Y, Jamshidi K, Tsuji H, Hyon S-H (1987) Macromolecules 20:906
Tsuji H, Horii F, Hyon S-H, Ikada Y (1991) Macromolecules 24:2719
Tsuji H, Hyon S-H, Ikada Y (1991) Macromolecules 24:5651
Tsuji H, Hyon S-H, Ikada Y (1991) Macromolecules 24:5657
Tsuji H, Hyon S-H, Ikada Y (1992) Macromolecules 25:2940
Tsuji H, Ikada Y (1992) Macromolecules 25:5719
Tsuji H, Horii, Nakagawa M, Ikada Y, Odani H, Kitamaru R (1992) Macromolecules 25:4114
Tsuji H, Ikada Y (1993) Macromolecules 26:6918
Brizzolara D, Cantow H-J, Diederichs K, Keller E, Domb A J (1996) Macromolecules 29:191
Serizawa T, Yamashita H, Fujiwara T, Kimura Y, Akashi M (2001) Macromolecules 34:1996
Decher G (1997) Science 277:1232
Arikawa Y, Serizawa T, Mukose T, Kimura Y, Akashi M, J Nanosci Nanotechnol in press
Serizawa T, Arikawa Y, Hamada K, Yamashita H, Fujiwara T, Kimura Y, Akashi M (2001) Macromolecules 36:1762
Serizawa T, Hashiguchi S, Akashi M (1999) Langmuir 23:5363
Serizawa T, Yamamoto K, Akashi M (1999) Langmuir 15:4682
Serizawa T, Ken-ichi H, Tatsuki K, Akashi M (2003) Angew Chem 115:1150 (2003) Angew Chem Int Ed 42:1118
Serizawa T, Ken-ichi H, Akashi M Nature (2004) 429:52
Ken-ichi H, Serizawa T, Akashi M (2005) Macromolecules, 38:6759
Sauerbrey G Z (1959) Phys 155:206
Amass W, Amass A, Tighe B (1998) Polym Int 47:89
Zhang J, Sato H, Tsuji H, Noda I, Ozaki Y (2005) Macromolecules 38:1822
Lu J, Peter J S, Lyman D M, Lai H –L, Leite M S, Tamada A J, Vacanti P J, Langer R, Mikos G A (2000) 21:1595
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Arikawa, Y., Serizawa, T., Mukose, T. et al. Controlled degradation of porous poly(lactide) stereocomplex films prepared by the selective extraction of co-assembled poly(vinyl alcohol). Polym. Bull. 58, 703–709 (2007). https://doi.org/10.1007/s00289-006-0699-8
Received:
Revised:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s00289-006-0699-8