Abstract
Gaseous ammonia treatments as well as thermal modification of timber are both applied to modify the surface colour of wood species. Physical and mechanical properties of solid wood after gaseous ammonia treatments have been so far scarcely investigated. Selected physical and mechanical properties, i.e., colour, equilibrium moisture content, wood density, bending strength, bending stiffness, and impact bending strength were investigated for oak, Norway spruce and Scots pine after gaseous ammonia treatment. Obtained data were compared with thermally modified timber data. While wood colour changes were comparable, most properties of the ammonia treated wood did not alter. There was no significant density change of ammonia treated wood; equilibrium moisture content changed moderately. Mechanical properties also remained within acceptable fluctuations. Results proved that gaseous ammonia treatment is a modification that improves the decorative value but has minimal effect on technologically relevant properties of solid wood. In contrast, property alterations of colour-equivalent thermally modified timber were much more pronounced, with possible limitations to some applications.
Zusammenfassung
Sowohl Ammoniakbehandlungen (Räuchern) als auch thermische Modifikation werden zur Farbmodifikation von Holzoberflächen eingesetzt. Physikalische und mechanische Eigenschaften von geräuchertem Holz wurden bisweilen selten untersucht. Ausgewählte physikalische und mechanische Kenngrößen, d.h. Farbe, Ausgleichsfeuchte, Holzdichte, Biegefestigkeit, Biegesteifigkeit und Schlagbiegefestigkeit wurden für Eiche, Fichte und Rotkiefer nach gasförmiger Ammoniakbehandlung untersucht. Die gemessenen Daten wurden mit Daten für thermisch modifiziertes Holz verglichen. Während die Holzfarbe vergleichbar war, änderten sich die meisten weiteren Eigenschaften von geräuchertem Holz nicht. Es gab keine signifikante Veränderung der Dichte und die Ausgleichsfeuchte änderte sich lediglich geringfügig. Auch die mechanischen Eigenschaften bewegten sich innerhalb üblicher Variationen. Die Ergebnisse zeigen, dass Räuchern ein Modifikationsverfahren ist, welches den dekorativen Wert des Holzes erhöht, während technologisch relevante Holzeigenschaften nicht beeinträchtigt werden. Im Vergleich dazu zeigt farblich ähnliches thermisch modifiziertes Holz wesentlich stärkere Veränderungen der Holzeigenschaften, welche für manche Anwendungen limitierend wirken können.
Similar content being viewed by others
References
Allegretti O, Cividinir R, Tessadri B (2008) Thermal treatment in saturated vapour pressure for spruce. In: Gard WF, van de Kuilen JWG (eds) Proceedings of conference COST E53, 29–30 October 2008. Delft, pp 125–134
Bariska M (1969) Plastifizierung des Holzes mit Ammoniak in Theorie und Praxis. Holz-Zent.bl 95(84):1309–1311
Bariska M (1975) Collapse phenomena in beechwood during and after NH3-impregnation. Wood Sci Technol 9:293–306
Berzin’š G, Wagenführ R, Steiger A (1970) Strukturveränderungen des Holzes beim Plastifizierungsvorgang. Holztechnologie 11(4):233–236
Berzin’š G (1972) Holzplastifizierung als Weg zur qualitätserhöhenden Werkstoffsubstitution. Holztechnologie 13(2):103–110
Besold G, Fengel D (1983a) Systematische Untersuchungen der Wirkung aggressiver Gase auf Fichtenholz, Teil 2: Veränderungen an den Polysacchariden und am Lignin. Holz Roh- Werkst 41:265–269
Besold G, Fengel D (1983b) Systematische Untersuchungen der Wirkung aggressiver Gase auf Fichtenholz, Teil 3: Sorptionsversuche, Festigkeitsprüfung und Erstellung eines Beurteilungsschemas. Holz Roh- Werkst 41:333–337
Boonstra MJ, Van Acker J, Tjeerdsma BF, Kegel EV (2007) Strength properties of thermally modified softwoods and its relation to polymeric structural wood constituents. Ann For Sci 64(7):679–690
Davidson RW, Baumgardt WG (1970) Plasticizing wood with ammonia—a progress report. For Prod J 20(3):19–25
DIN 52182 (1976) Testing of wood; determination of density
DIN 52183 (1977) Testing of wood; determination of moisture content
DIN 52186 (1978) Testing of wood; bending test
DIN 52189 (1981) Testing of wood; determination of impact bending strength
Esteves B, Marques AV, Domingos I, Pereira H (2007) Influence of steam heating on the properties of pine (Pinus pineaster) and eucalypt (Eucalyptus globulus) wood. Wood Sci Technol 41:193–207
Esteves BM, Domingos IJ, Pereira HM (2008a) Pine wood modification by heat treatment in air. Bioresources 3(1):142–154
Esteves B, Marques AV, Domingos I, Pereira H (2008b) Heat-induced colour changes of pine (Pinus pinaster) and eucalypt (Eucalyptus globulus) wood. Wood Sci Technol 42:369–384
Fengel D, Wegener G (1984) Wood—chemistry, ultrastructure, reactions. De Gruyter, Berlin
Graf G, Koch H, Schiene R, Schuster E (1971) Herstellung und Festigkeit von Platten aus ammoniakplastifizierten Fasern (I). Holztechnologie 12(4):235–238
Graf G, Koch H, Schiene R, Schuster E (1972) Herstellung und Festigkeit von Platten aus ammonakplatifizierten Fasern (II). Holztechnologie 13(3):152–155
González-Peña MM, Hale MDC (2009a) Colour in thermally modified wood of beech, Norway spruce and Scots pine. Part 1: Colour evolution and colour change. Holzforschung 63:385–393
González-Peña MM, Hale MDC (2009b) Colour in thermally modified wood of beech, Norway spruce and Scots pine. Part 2: Property prediction from colour changes. Holzforschung 63:394–401
Hill CAS (2006) Wood modification—chemical, thermal and other processes. Wiley, New York
Kalnin’š AJ, Darzin’š TA, Jukna AD, Berzin’š GV (1967) Physikalisch-mechanische Eigenschaften mit Ammoniak chemisch plastifizierten Holzes. Holztechnologie 8(1):23–28
Kalnin’š A, Berzin’š G, Skrupskis W, Rumba A (1969) Chemisch plastifiziertes Holz anstelle von Buntmetallen und importiertem Hartholz. Holztechnologie 10(1):17–23
Oniśko W, Matejak M (1971) Einfluß 25 % iger Ammoniaklösung auf die physikalischen und mechanischen Eigenschaften des Holzes. Holztechnologie 12(1):45–54
Parameswaran N, Roffael E (1984) Kenntnisstand und Untersuchungsergebnisse zur Wirkung von Ammoniak auf Holzspäne. Holz Roh- Werkst 42:327–333
Parham RA, Davidson RW, de Zeeuw CH (1971) Radial-tangential shrinkage of ammonia-treated loblolly pine wood. Wood Sci 4(3):129–136
Patzelt M, Stingl R, Teischinger A (2002) Thermische Modifikation von Holz und deren Einfluß auf ausgewählte Holzeigenschaften. In: Teischinger A, Stingl R (eds) Lignovisionen Band 3: Modifiziertes Holz: Eigenschaften und Märkte. Schriftenreihe des Instituts für Holzforschung und des Verband Holzwirte Österreichs, Boku Vienna, pp 101–147
Sailer M, Rapp AO, Leithoff H, Peek RD (2000) Vergütung von Holz durch Anwendung einer Öl-Hitzebehandlung. Holz Roh- Werkst 58:15–22
Seeling U, Ohnesorge D, Helzle C, Burgbacher C, Németh R, Tolvaj L, Teischinger A, Hansmann C, Mitteramskogler H, Huber H, Oliver JV, Abián MA, Pons L, Custodio R (2007) Red heartwood handbook. University of Freiburg, Institute for Forest Utilisation and Work. Science, Freiburg
Stamm AJ (1955) Swelling of wood and fiberboards in liquid ammonia. For Prod J 5(6):413–416
Sundqvist B, Morén T (2002) The influence of wood polymers and extractives on wood color induced by hydrothermal treatment. Holz Roh- Werkst 60:375–376
Tinkler CK (1921) “Fumed” oak and natural brown oak. Biochem J 15(4):477–486
Weigl M, Pöckl J, Müller U, Pretzl H, Grabner M (2007) UV-resistance of ammonia treated wood. In: Hill CAS, Jones D, Militz H, Ormondroyd GA (eds) 3rd European conference on wood modification, 15–16 October 2007. Cardiff, pp 209–212
Weigl M, Müller U (2009) On the physical and mechanical properties of gas phase ammonia treated wood. In: Englund F, Hill CAS, Militz H, Segerholm BK (eds) Proceedings of the 4th European conference on wood modification, 27–29 April 2009. Stockholm, pp 483–486
Weigl M, Kandelbauer A, Hansmann C, Pöckl J, Müller U, Grabner M (2009a) Application of Natural Dyes in the Coloration of Wood. In: Bechtold T, Mussak R (eds) Handbook of natural colorants. Wiley, New York, pp 277–313
Weigl M, Pöckl J, Grabner M (2009b) Selected properties of gas phase ammonia treated wood. Eur J Wood Prod 67:103–109
Welzbacher CR, Brischke C, Rapp AO (2007) Influence of treatment temperature and duration on selected biological, mechanical, physical and optical properties of thermally modified timber. Wood Mater Sci Eng 2:66–76
Yatsu LA, Calamari TA, Benerito RR (1986) Conversion of cellulose I to stable cellulose III. Tex Res J 56(7):419–424
Acknowledgements
This study was supported by the Austrian government and the federal governments of Lower Austria, Upper Austria, and Carinthia supporting the Austrian COMET programme. The authors wish to acknowledge support from Murat Gündüz concerning laboratory work.
The authors declare that they have no conflict of interest.
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Weigl, M., Müller, U., Wimmer, R. et al. Ammonia vs. thermally modified timber—comparison of physical and mechanical properties. Eur. J. Wood Prod. 70, 233–239 (2012). https://doi.org/10.1007/s00107-011-0537-z
Received:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s00107-011-0537-z