Conclusions
-
1.
Carbonitriding at 800°C and heat treatment of flat blades of supershears and guillotines from steel 40Kh with subsequent grinding of the faces to a specific depth provides self-sharpening of the blades in operation.
-
2.
In order to provide a self-sharpening regime after the creation of the diffusion layer on the faces of a blade and a hardening heat treatment, a part of the layer of the “soft” face is ground off to a hardness much lower than that of the surface of the “hard” face.
-
3.
The structural strength of the blades is provided by optimum regimes of carbonitriding, quenching; and double tempering and raising the toughness of the “soft” face by a partial removal of the surface “hard” layer.
Similar content being viewed by others
References
V. N. Tkachev, B. M. Fishtein, V. D. Vlasenko, and V. A. Ulanov,Methods for Increasing the Service Life of Machine Parts [in Russian], Mashinostroenie, Moscow (1971).
L. P. Karpov, “Carbonitriding with the use of triethanolamine at 800°C,”Metalloved. Term. Obrab. Met., No. 2, 8–12 (1998).
A Method for Carbonitriding Steel. RF Patent No. 2082820. 27.06.97 [in Russian].
V. D., Kal'ner (ed.),Control over the Quality of Heat Treatment of Steel Semiproducts and Parts. A Handbook [in Russian], Mashinostroenie, Moscow (1984).
Author information
Authors and Affiliations
Additional information
Translated from Metallovedenie i Termicheskaya Obrabotka Metallov, No. 6, pp. 16–19, June, 1999.
Rights and permissions
About this article
Cite this article
Karpov, L.P. Use of carbonitriding for self-sharpening of tools in service. Met Sci Heat Treat 41, 250–252 (1999). https://doi.org/10.1007/BF02468238
Issue Date:
DOI: https://doi.org/10.1007/BF02468238