Conclusions
A study was made of the processes of electroless plating of alumina powders with nickel and copper. Electroless nickel and copper plating with full pretreatment was performed at room temperature. In nickel plating by the process investigated the number of pretreatment operations can be reduced by raising the solution temperature to 50–55°C, although nickel plating with full pretreatment is to be preferred from a practical point of view. The concentrated solutions investigated are suitable for the application of nickel and copper layers of considerable thickness to alumina powder particles.
Similar content being viewed by others
Literature cited
B. S. Skidan, G. A. Fomina, and I. A. Shepilov, “A study of the effect of processing factors on the properties of alumina-molybdenum cermets,” Poroshk. Metal., No. 5, 93–96 (1978).
G. G. Gnesin, I. I. Osipova, V. P. Yaroshenko, and G. D. Rontal', “Optimization of the properties of a tool material based on silicon nitride,” Poroshk. Metall., No. 2, 48–52 (1978).
L. T. Gordeeva, K. N. Gedgovd, A. I. Krasovskii, V. I. Morozov, et al., “Effect of processing parameters on some properties of detonation-deposited alumina coatings,” Poroshk. Metall., No. 1, 88–91 (1978).
N. G. Baranov, Yu. N. Semenov, and N. P. Brodnikovskii, “Effect of structure on the frictional behavior of a copper-titanium-carbide composite,” Poroshk. Metall., No. 1, 37–40 (1977).
I. M. Fedorchenko, Yu. A. Popchenko, L. V. Zabolotnyi, et al., “Self-lubricating composite materials and their frictional characteristics,” Poroshk. Metall., No. 1, 78–82 (1977).
Yu. A. Kharlamov, L. I. Kalinin, V. V. Rishin, et al., “Detonation deposition of hard-alloy coatings from a mechanical mixture of fine powders,” Poroshk. Metall., No. 4, 41–46 (1978).
W. J. Wilson, M. F. Browning, and J. M. Blocher, Jr., “Vapor deposition of wear-resistant coatings,” U. S. Dept. Com., Nat. Bur. Std. Spec. Publ. No. 452 (1976), pp. 151–167.
A. Ya. Greiman and Yu. A. Sidorenko, “Preparation of composites for sintered materials by the electroless plating method,” in: New and Advanced Technology [in Russian], Vyshéishaya Shkola, Minsk (1969), pp. 284–286.
A. N. Yagubets and A. N. Andreeva, “An electroless method for plating whiskers with nickel” Izv. Akad. Nauk MSSR, 88–91 (1976).
V. V. Vashchenko, et al., “Solution for the electroless plating of aluminum powder,” Inventor's Certificate No. 436891; Byull. Izobret., No. 27 (1974).
V. Ya. Omel'chenko, T. A. Plotnikova, and L. L. Kuz'min, “Low-temperature electroless plating of disperse materials with nickel,” Izv. Vyssh. Uchebn. Zaved., Khim. Khim. Tekhnol.,16, 1299–1300 (1973).
L. I. Kadaner, Handbook of Electroplating [in Russian], Tekhnika, Kiev (1976), p. 253.
T. F. Yudina, “An investigation into the technology of electroless plating of very fine powder materials with copper,” Author's Abstract of Candidate's Dissertation, Ivanovo (1970).
Author information
Authors and Affiliations
Additional information
Translated from Poroshkovaya Metallurgiya, No. 5(209), pp. 14–16, May, 1980.
Rights and permissions
About this article
Cite this article
Mel'nikov, V.G., Zamyatina, N.I., Yudina, T.F. et al. Electroless deposition of metals on alumina powders. Powder Metall Met Ceram 19, 307–309 (1980). https://doi.org/10.1007/BF00791549
Revised:
Issue Date:
DOI: https://doi.org/10.1007/BF00791549