Conclusions
-
1.
A heating rate of 20 deg/h ensures good formability for deep drawing of steel stabilized with aluminum.
-
2.
The aluminum content affects the texture formation and thus the changes in the mechanical properties during annealing. Better mechanical properties and crystallographic texture favorable for good formability were obtained for the steel with 0.055% Al than for the steel with 0.012% Al.
Similar content being viewed by others
Literature cited
D. Blickwede, Trans. Quart.,61, No. 4, 653 (1969).
M. L. Drobinskii and V. Yu. Novikov, "Effect of preliminary annealing on recrystallization of steel 08Yu," Izv. Vyssh. Uchebn. Zaved., Chern. Metallurgiya, No. 5, 128 (1973).
P. Richards, J. Austral. Inst. Metals,12, No. 1, 2 (1967).
P. Richards, J. Austral. Inst. Metals,14, 313 (1968).
A. A. Vostrikov, V. P. Gubchevskii, and É. D. Nemkina, "Normal anisotropy and texture of cold-rolled sheet steel," Stal', No. 11, 1026 (1972).
A. A. Vostrikov, V. P. Gubchevskii, and É. D. Nemkina, "Formation of texture during deformation of low-carbon steels," Fiz. Met. Metalloved.,35, No. 4, 832 (1973).
M. P. Mishin, M. I. Kolov, and B. I. Smirnov, "Recrystallization annealing of coils of wide automotive sheet steel," Stal', No. 2, 155 (1973).
Additional information
Magnitogorsk Metallurgical Combine. Translated from Metallovedenie i Termicheskaya Obrabotka Metallov, No. 4, pp. 68–70, April, 1977.
Rights and permissions
About this article
Cite this article
Gubchevskii, V.P., Nemkina, É.D., Mishin, M.P. et al. Effect of annealing conditions on the properties of steel 08Yu. Met Sci Heat Treat 19, 323–325 (1977). https://doi.org/10.1007/BF00700824
Issue Date:
DOI: https://doi.org/10.1007/BF00700824