Conclusions
-
1.
Examination of the fatigue of fiber glass plastic pipes in loading with the sinusoidal cycle can be replaced with an error of up to 10% by tests with the right-angled cycle in equipment of simple design.
-
2.
The endurance limit in the right-angled cycle is lower than in the sinusoidal cycle. Therefore, in testing the pipes it is necessary to avoid sharp changes in internal pressure if the winding angle is αi> 15°.
-
3.
The tangential stress corresponding (with an error of up to 15%) to the endurance limit in the right-angled load cycle can be determined on the basis of acoustic emission in static internal pressure loading.
Similar content being viewed by others
Literature cited
M. Nowak, “Examination of fatigue endurance of composite laminate pipes,” Pr. Nauk. Politech. Wroclaw., No. 12, 70 (1980).
W. Loertsch, “Plastic pipes loaded with static pulsed internal pressure,” Kunststoffe, No. 6, 460–464 (1965).
C. E. Kirstein, “Behavior of thermoplastic pipes in dynamic loading,” in: 2nd Colloquium on Plastics, Stuttgart (1971), p. 7.
C. E. Kirstein, “Dynamic loading of plastic pipes,” in: 3rd Colloquium on Plastics, Stuttgart (1973), p. 14.
G. Schonefeld and S. Wintergerst, “Effect of bursting and peak pressure on drinking water pipes made of hard PVC in warm places,” Maschinenschaden, No. 5, 183–189 (1970).
V. S. Strelyaev and L. L. Sachkovskaya, “Propagation of shear cracks in fiber glass plastics in cyclic loading,” Zavod. Lab., No. 10, 1288–1293 (1961).
P. Boess, “Pressure surge problems, investigations in laboratory and on equipment in service,” Gas Wasserfach, No. 22, 548–552 (1957).
V. P. Vlasov, “Resistance of pipes made of hard polyvinyl chloride to alternating internal pressure,” Mekh. Polim., No. 4, 747–749 (1967).
V. N. Mozhin, “Equipment for testing fatigue of plastics in the biaxial stress state,” Zavod. Lab., No. 4, 498–499 (1972).
A. S. Aistov, “Equipment for testing large-diameter pipes with pulsed internal pressure,” Zavod. Lab., No, 1, 108–109 (1975).
V. A. Sherstnev and A. Ya. Gol'dman, “Equipment for testing fatigue of polymer materials in a plane stress state,” Probl. Prochn., No. 12, 111–113 (1976).
O. G. Tsyplakov, Ship Pipelines Made of Fiber Glass Plastic [in Russian], Leningrad (1967).
T. Kilian, “Equipment for testing fatigue endurance of laminate pipes in right-angled internal pressure cyclic loading,” Pr. Nauk. Politech. Wroclaw., No. 38, 35–55 (1978).
K. Oberbach and G. Hesse, “Effect of loading frequency and form on the vibration behavior of plastics,” Materialpruefung, No. 6, 173–178 (1972).
A. Puck, “Loading and deformation of GFK multilayer bonded structural members,” Kunststoffe, No. 4, 284–293 (1967); No. 7, 573–582 (1967).
M. Ya. Tutans and Yu. S. Urzhumtsev, “Prediction of the process of failure of glass-reinforced plastics by the seismoacoustic method,” Mekh. Polim., No. 3, 421–429 (1971).
I. Jerzyk and M. Kumosa, “Effect of the winding angle of glass fibers on the nature of acoustic emission in pipes made of an epoxy-glass laminate,” Report No. 23, Wroclaw Polytechnical Institute (1983).
N. E. Sarkisyan, “Anisotropy of fatigue strength of anisotropic glass-fiber reinforced materials,” Izv. Akad. Nauk Arm. SSR, Mekh., No. 2, 59–70 (1971).
Author information
Authors and Affiliations
Additional information
Translated from Mekhanika Kompozitnykh Materialov, No. 4, pp. 633–641, July–August, 1985.
Rights and permissions
About this article
Cite this article
Nowak, M., Jerzyk, I. Effect of the characteristics of sinusoidal and rectangular cycles on the endurance limit of pipes of a laminated epoxy fiber glass plastic. Mech Compos Mater 21, 432–439 (1986). https://doi.org/10.1007/BF00610891
Received:
Issue Date:
DOI: https://doi.org/10.1007/BF00610891