Abstract
Ni-MgO catalysts have been widely applied for carbon dioxide reforming (CDR) reaction due to their ability of anti-carbon formation. However, activation of Ni-MgO catalyst consumes considerable energy because of its very low reducibility. In this study, ZrO2, CeO2, and CeO2-ZrO2 promoted Ni-MgO catalysts were prepared via a facile coprecipitation method and applied to the CDR reaction. Among the prepared catalysts, the ZrO2-promoted Ni-MgO catalyst showed the highest methane conversion. The high catalytic performance of the ZrO2-promoted Ni-MgO catalyst is mainly due to easier reducibility, high Ni dispersion, and high specific surface area.
Similar content being viewed by others
References
W.-J. Jang, D.-W. Jeong, J.-O. Shim and H.-S. Roh, Int. J. Hydrogen Energy, 38, 4508 (2013).
A. T. Ashcroft, A. K. Cheetham, M. L. H. Green and P. D. F. Vernon, Nature, 352, 225 (1991).
N. Rahemi, M. Haghighi, A. A. Babaluo and M. F. Jafari, Korean J. Chem. Eng., 31, 1553 (2014).
G. Valderrama, A. Kiennemann and M. R. Goldwasser, J. Power Sources, 195, 1765 (2010).
S. Özkara-Aydinoğlu, Int. J. Hydrogen Energy, 35, 12821 (2010).
M. C. J. Bradford and M. A. Vannice, J. Catal., 173, 157 (1998).
H.-S. Roh and K.-W. Jun, Catal. Surv. Asia, 12, 239 (2008).
H.-S. Roh, H. S. Potdar and K.-W. Jun, Catal. Today, 93, 39 (2004).
H.-S. Roh, H. S. Potdar, K.-W. Jun, J.-W. Kim and Y.-S. Oh, Appl. Catal. A-Gen., 276, 231 (2004).
M. H. A. Shiraz, M. Rezaei and F. Meshkani, Korean J. Chem. Eng., 33, 3359 (2016).
J. Wei and E. Iglesia, J. Catal., 224, 370 (2004).
J. Wei and E. Iglesia, J. Phys. Chem. B, 108, 4094 (2004).
J. Wei and E. Iglesia, Phys. Chem. Chem. Phys., 6, 3754 (2004).
J. Wei and E. Iglesia, J. Catal., 225, 116 (2004).
J. Wei and E. Iglesia, J. Phys. Chem. B, 108, 7253 (2004).
S. A. Theofanidis, V. V. Galvita, H. Poelman and G. B. Marin, ACS Catal., 5, 3028 (2015).
K.-Y. Koo, H.-S. Roh, Y.-T. Seo, D.-J. Seo, W.-L. Yoon and S.-B. Park, Appl. Catal. A-Gen., 340, 183 (2008).
K.-W. Jun, H.-S. Roh and K. V. R. Chary, Catal. Surv. Asia, 11, 97 (2007).
Y. H. Hu and E. Ruckenstein, J. Catal., 184, 298 (1999).
Y. H. Wang, H. M. Liu and B. Q. Xu, J. Mol. Catal. A: Chem., 299, 44 (2009).
Y. H. Hu and E. Ruckenstein, Langmuir, 13, 2055 (1997).
Y. H. Hu and E. Ruckenstein, Catal. Rev., 44, 423 (2002).
W.-J. Jang, J.-O. Shim, H.-M. Kim, S.-Y. Yoo and H.-S. Roh, Catal. Today, 324, 15 (2019).
J.-O. Shim, W.-J. Jang, K.-W. Jeon, D.-W. Lee, H.-S. Na, H.-M. Kim, Y.-L. Lee, S.-Y. Yoo, B.-H. Jeon, H.-S. Roh and C.-H. Ko, Appl. Catal. A-Gen., 563, 163 (2018).
S. Wang and G. Q. Lu, Appl. Catal. B-Env., 19, 267 (1998).
S. Zhang, S. Muratsugu, N. Ishiguro and M. Tada, ACS Catal., 3, 1855 (2013).
R. Debek, M. E. Galvez, F. Launay, M. Motak, T. Grzybek and P. D. Costa, Int. J. Hydrogen Energy, 41, 11611 (2016).
L. Yao, J. Zhu, X. Peng, D. Tong and C. Hu, Int. J. Hydrogen Energy, 38, 7268 (2013).
D. Liu, Y. Quek, W. N. E. Cheo, R. Lau, A. Borgna and Y. Yang, J. Catal., 266, 380 (2009).
E. C. Faria, R. C. R. Neto, R. C. Colman and F. B. Noronha, Catal. Today, 228, 138 (2014).
V. Shanmugam, R. Zapf, S. Neuberg, V. Hessel and G. Kolb, Appl. Catal. B-Env., 203, 859 (2017).
G. J. Hutchings and J. C. Védrine, Heterogeneous catalyst preparation, M. Baerns, Eds., Springer Berlin Heidelberg, Berlin, Heidelberg, 215 (2004).
A. Platon, H.-S. Roh and D. L. King, Top. Catal., 46, 374 (2007).
F. A. J. Al-Doghachi, U. Rashid and Y. H. Taufiq-Yap, RSC Adv., 6, 10372 (2016).
A. Luengnaruemitchai, C. Pojanavaraphan, A. Kumyam, C. Thunyaratchatanon and E. Gulari, Int. J. Hydrogen Energy, 44, 1686 (2019).
A. Arslan and T. Dogu, Int. J. Hydrogen Energy, 41, 16752 (2016).
H.-S. Roh, K.-W. Jun, W.-S. Dong, J.-S. Chang, S.-E. Park and Y.-I. Joe, J. Mol. Catal. A-Chem., 181, 137 (2002).
H.-M. Kim, W.-J. Jang, S.-Y. Yoo, J.-O. Shim, K.-W. Jeon, H.-S. Na, Y.-L. Lee, B.-H. Jeon, J.-W. Bae and H.-S. Roh, Int. J. Hydrogen Energy, 43, 262 (2018).
Y. Qian, S. Liang, T. Wang, Z. Wang, W. Xie and X. Xu, Catal. Commun., 12, 851 (2011).
I.-H. Choi, K.-R. Hwang, K.-Y. Lee and I.-G. Lee, Int. J. Hydrogen Energy, 44, 180 (2019).
M. Miyamoto, A. Hamjima, Y. Oumi and S. Uemiya, Int. J. Hydrogen Energy, 43, 730 (2018).
M. Rezaei and S. M. Alavi, Int. J. Hydrogen Energy, 44, 16516 (2019).
R. Debek, M. Radlik, M. Motak, M. E. Galvez, W. Turek, P.D. Costa and T. Grzybek, Catal. Today, 257, 59 (2015).
Y. Yang, J. Liu, W. Shen, J. Li and I. L. Chien, Energy, 158, 820 (2018).
M. Khajenoori, M. Rezaei and F. Meshkani, Chem. Eng. Tech., 37, 957 (2014).
F. Meshkani, M. Rezaei and M. Andache, J. Ind. Eng. Chem., 20, 1251 (2014).
M. Usman and W. M. A. W. Daud, RSC Adv., 6, 38277 (2016).
Acknowledgements
This work was supported by Next Generation Carbon Upcycling Project (Project No. 2017M1A2A2044372) through the National Research Foundation (NRF) funded by the Ministry of Science and ICT, Republic of Korea.
Author information
Authors and Affiliations
Corresponding authors
Rights and permissions
About this article
Cite this article
Kim, BJ., Jeon, KW., Na, HS. et al. Reducible oxide (CeO2, ZrO2, and CeO2-ZrO2) promoted Ni-MgO catalysts for carbon dioxide reforming of methane reaction. Korean J. Chem. Eng. 37, 1130–1136 (2020). https://doi.org/10.1007/s11814-020-0551-0
Received:
Revised:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s11814-020-0551-0