Fig. 2From: Material Solutions to Increase the Information Density in Mold-Based Production SystemsEBSD-images of 1.2343 Standard (a) powder particle with ca. 5% RA (red), (b) as built without preheating with ca. 18% RA (yellow), (c) with preheating at 500 °CBack to chapter page