Growth of nanocrystalline PbS within a glass M. MukherjeeA. DattaD. Chakravorty Articles 31 January 2011 Pages: 2507 - 2510
Rapid thermal recrystallization of amorphous silicon films G. D. BeshkovD. B. DimitrovE. Vlaev Articles 31 January 2011 Pages: 2511 - 2514
Melt-infiltration processing of TiC/Ni3Al composites K. P. PlucknettP. F. BecherR. Subramanian Articles 31 January 2011 Pages: 2515 - 2517
Low temperature synthesis of ultrafine Pb(Zr, Ti)O3 powder by sol-gel combustion J. SchäferW. SigmundF. Aldinger Articles 31 January 2011 Pages: 2518 - 2521
Growth of high-quality Bi2Sr2CaCu2Oz crystal and characterization H. FaqirG. VacquierY. Syono Articles 31 January 2011 Pages: 2522 - 2525
Phase identification and superconductivity transitions in Sr-doped Pr1.85Ce0.15CuO4+δ A. VarelaM. Vallet-RegíJ. M. González-Calbet Articles 26 July 2012 Pages: 2526 - 2532
Structural studies of diamond thin films grown from dc arc plasma L. C. NistorJ. Van LanduytE. D. Obraztsova Articles 31 January 2011 Pages: 2533 - 2542
Scanning tunneling microscope study of polyacrylonitrile-based carbon fibers Dongxia ShiNing LiuZhen Ji Articles 31 January 2011 Pages: 2543 - 2547
On the formation of solid state crystallized intrinsic polycrystalline germanium thin films Zhiguo MengZhonghe JinMan Wong Articles 31 January 2011 Pages: 2548 - 2551
Quantum size effect of ZnSe microcrystal-doped SiO2 glass thin films prepared by RF-sputtering method Masayuki HayashiTakafumi IwanoKazuyuki Hirao Articles 31 January 2011 Pages: 2552 - 2558
Shear faults and dislocation core structures in B2 CoAl C. VailhéD. Farkas Articles 31 January 2011 Pages: 2559 - 2570
Fatigue crack initiation at Nd-rich particles in an Nd containing high temperature titanium alloy J. F. LeiQ. J. WangZ. Q. Hu Articles 31 January 2011 Pages: 2571 - 2574
Crystallization of hafnia and zirconia during the pyrolysis of acetate gels Masatomo YashimaTaka Aki KatoMasahiro Yoshimura Articles 31 January 2011 Pages: 2575 - 2583
Spinel solid solutions in the systems MgAl2O4–ZnAl2O4 and MgAl2O4–Mg2TiO4 M. A. PetrovaG. A. MikirtichevaV. F. Popova Articles 31 January 2011 Pages: 2584 - 2588
Phase instability in ZrO2–NiAl functionally graded materials Yi Rong HeVidya SubramanianJohn J. Lannutti Articles 31 January 2011 Pages: 2589 - 2593
Phase structure and thermal evolution in coating films and powders obtained by sol-gel process: Part II. ZrO2–2.5 mole% Y2O3 R. CarusoE. BenavídezA. Serquis Articles 31 January 2011 Pages: 2594 - 2601
A structural study of amorphous alkoxide-derived lead titanium complexes Barbara MaličIztok ArčonAlojz Kodre Articles 31 January 2011 Pages: 2602 - 2611
Domain structures in Pb(Zr, Ti)O3 and PbTiO3 thin films L. D. MadsenE. M. GriswoldL. Weaver Articles 31 January 2011 Pages: 2612 - 2616
Processing and characterization of lead magnesium tantalate ceramics Mehmet A. AkbasPeter K. Davies Articles 26 July 2012 Pages: 2617 - 2622
Elastic properties of tetragonal PbTiO3 single crystals by Brillouin scattering A. G. KalinichevJ. D. BassD. A. Payne Articles 31 January 2011 Pages: 2623 - 2627
Impedance spectroscopy of SrBi2Ta2O9 and SrBi2Nb2O9 ceramics correlation with fatigue behavior Tze Chiun ChenChai Liang ThioSeshu B. Desu Articles 31 January 2011 Pages: 2628 - 2637
Estimation of Weibull parameter with a modified weight function B. K. Chandrasekhar Articles 31 January 2011 Pages: 2638 - 2642
On the fluctuation field in multidomain barium hexaferrite particles J. M. GonzálezAnit K. GiriJ. L. Vicent Articles 31 January 2011 Pages: 2643 - 2647
Giant magnetoresistance in bulk La0.6Mg0.4MnO3 Yadong LiX. F. DuanC. F. Zhu Articles 31 January 2011 Pages: 2648 - 2650
Decomposition behavior of Ln2Mn4/3W2/3O7 (Ln = Eu and Er) in reducing atmosphere and their thermodynamic properties Taroh AtsumiNaoki Kamegashira Articles 31 January 2011 Pages: 2651 - 2656
Reaction path in the magnesium thermite reaction to synthesize titanium diboride V. SundaramK. V. LoganR. F. Speyer Articles 31 January 2011 Pages: 2657 - 2664
Strontium and calcium zirconyl citrates as precursors for the low-temperature synthesis of SrZrO3 and CaZrO3 fine powders M. RajendranM. Subba Rao Articles 31 January 2011 Pages: 2665 - 2672
Investigation of a new fracture mechanics specimen for thin film adhesion measurement Maarten P. de BoerMichael KrieseWilliam W. Gerberich Articles 31 January 2011 Pages: 2673 - 2685
A sequential Raman analysis of the growth of diamond films on silicon substrates in a microwave plasma assisted chemical vapor deposition reactor L. FayetteB. MarcusG. Lucazeau Articles 31 January 2011 Pages: 2686 - 2698
Pulsed laser deposition of KNbO3 thin films M. J. MartínJ. E. AlfonsoP. J. Chandler Articles 31 January 2011 Pages: 2699 - 2706
Nanoindentation measurements of amorphous carbon coatings Ashok V. KulkarniBharat Bhushan Articles 31 January 2011 Pages: 2707 - 2714
Effect of Nd content on the magnetic properties and crystallographic alignment of Fe–Nd–B–Al sintered magnets W. KaszuwaraM. LeonowiczH. A. Davies Articles 31 January 2011 Pages: 2715 - 2718
Preparation of nanocrystalline copper by electrodeposition S. BandyopadhyayD. Chakravorty Articles 31 January 2011 Pages: 2719 - 2724
Does the shear-lag model apply to random fiber networks? V. I. RäisänenM. J. AlavaR. M. Nieminen Articles 31 January 2011 Pages: 2725 - 2732
In situ mass spectrometry during diamond chemical vapor deposition using a low pressure flat flame C. A. WoldenR. F. DavisJ. T. Prater Articles 31 January 2011 Pages: 2733 - 2742
Camber development during cofiring Ag-based low-dielectric-constant ceramic package Jau Ho JeanChia Ruey Chang Articles 31 January 2011 Pages: 2743 - 2750
Schwertmannite: A unique mineral, contains a replaceable ligand, transforms to jarosites, hematites, and/or basic iron sulfate R. Joseph Barham Articles 31 January 2011 Pages: 2751 - 2758
Photo-oxidatively self-cleaning transparent titanium dioxide films on soda lime glass: The deleterious effect of sodium contamination and its prevention Y. PazA. Heller Articles 31 January 2011 Pages: 2759 - 2766
Iron-silica and nickel-silica nanocomposites prepared by high energy ball milling Anna CorriasGuido EnnasDaniela Zedda Articles 31 January 2011 Pages: 2767 - 2772
Studies on age-hardening characteristics of ceramic particle/matrix interfaces in Al–Cu–SiCp composites using ultra low-load-dynamic microhardness measurements B. DuttaM. K. Surappa Articles 31 January 2011 Pages: 2773 - 2778
Preparation and characterization of Nd3+ and Er3+-doped silica sol-gel coatings by Rutherford backscattering spectroscopy and spectroscopic ellipsometry S. BruynoogheA. ChabliG. Leflem Articles 31 January 2011 Pages: 2779 - 2783
Compensation phenomena in oil-resin mixtures: A new dielectric approach to percolative processes O. PagésA. LamureD. Craig Articles 31 January 2011 Pages: 2784 - 2793
An alternative analysis of water vapor and gas transport in polyimide films H. OuyangSanboh Lee Articles 31 January 2011 Pages: 2794 - 2798
The nature of residues following the ashing of arsenic implanted photoresist Clifton W. DraperChuck W. PearceSteven L. Bernasek Articles 31 January 2011 Pages: 2799 - 2808