Oxidation Behavior of Ti--50Al Intermetallics with Thin TiAl3 Film at 1000°C M. S. ChuS. K. Wu OriginalPaper Pages: 1 - 13
Scaling of Carbon Steel in Simulated Reheat Furnace Atmospheres V. H. J. LeeB. GleesonD. J. Young OriginalPaper Pages: 15 - 31
The Role of Oxygen Uptake and Scale Formation on the Embrittlement of Vanadium Alloys B. A. PintJ. R. DiStefano OriginalPaper Pages: 33 - 55
Study of Carbide Transformations during High-Temperature Oxidation of Nickel-Base Superalloys P. BerthodC. VébertC. Rapin OriginalPaper Pages: 57 - 72
In-situ Measurement of the Thickness of Aluminum Oxide Scales at High Temperature Sang-Shin LeeShin-Kyu SunKi-Ju Kang OriginalPaper Pages: 73 - 85
The Influence of Temperature on Oxide-Scale Formation during Erosion--Corrosion Rikard NorlingAnders Nylund OriginalPaper Pages: 87 - 111
Interfacial Segregation, Pore Formation, and Scale Adhesion on NiAl Alloys P.Y. HouK. Priimak OriginalPaper Pages: 113 - 130