Morphology of oxide scales formed on titanium G. BertrandK. JarrayaJ. M. Chaix OriginalPaper Pages: 1 - 19
Sulfidation properties of an Fe-26.6 at.% Cr alloy at temperatures of 973–1173 K in H2S-H2 atmospheres at sulfur Pressures 104–10−6 Pa T. NaritaW. W. Smeltzer OriginalPaper Pages: 39 - 55
Sulfidation mechanism of an Fe-26.6 at.% Cr alloy at temperatures 973–1173 K in H2S-H2 atmospheres at sulfur pressures 104–10−6 Pa T. NaritaW. W. Smeltzer OriginalPaper Pages: 57 - 69
A high-temperature oxidation-resistant Fe-Mn-Al-Si alloy Rosie WangMark J. StraszheimRobert A. Rapp OriginalPaper Pages: 71 - 79
In situ SEM study of the high-temperature oxidation of an Fe-Mn-Al-Si alloy Helmut ErhartRosie WangRobert A. Rapp OriginalPaper Pages: 81 - 88
In situ observation of whiskers, pyramids and pits during the high-temperature oxidation of metals G. M. RaynaudR. A. Rapp OriginalPaper Pages: 89 - 102