Theoretical strength of solids: recent results and applications J. Pokluda OriginalPaper 16 May 2012 Pages: 575 - 582
Assessment of the In-Service Degradation of Pipeline Steel by Destructive and Nondestructive Methods Yu. V. Mil’manH. M. NykyforchynL. V. Mordel’ OriginalPaper 17 May 2012 Pages: 583 - 589
Anisotropy of the Mechanical Properties of Degraded 15Kh1М1F Steel After Its Operation in Steam Pipelines of Thermal Power Plants О. Z. StudentH. V. Krechkovs’ka OriginalPaper 17 May 2012 Pages: 590 - 597
Effect of hydrogenation of the walls of oil-and-gas pipelines on their soil corrosion and service life O. V. HembaraO. E. Andreikiv OriginalPaper 18 May 2012 Pages: 598 - 607
Resistance of steels of railroad wheels to corrosion-fatigue fracture I. M. AndreikoV. V. KulykO. P. Ostash OriginalPaper 18 May 2012 Pages: 608 - 612
Complex method for checking physicomechanical characteristics of materials of metalworks O. M. KarpashE. R. DotsenkoM. O. Karpash OriginalPaper 17 May 2012 Pages: 613 - 620
Application of Fractal Geometry to the Problems of Prediction of the Residual Service Life of Aircraft Structures M. V. KaruskevychI. M. Zhuravel’T. P. Maslak OriginalPaper 17 May 2012 Pages: 621 - 626
Investigation of the Initial Stage of Kinking of an Interface Crack at an Angular Point of the Interface of Two Media M. V. DudykYu. V. Dikhtyarenko OriginalPaper 17 May 2012 Pages: 627 - 635
Monitoring of the fatigue of d16aт alloy according to the characteristics of deformation surface pattern S. R. IgnatovichS. S. Yutskevich OriginalPaper 18 May 2012 Pages: 636 - 643
Specific Features of the Formation of Structures in 60Kh2N4GМF Precipitation-Hardening Steel T. S. SkobloV. М. Vlasovets OriginalPaper 17 May 2012 Pages: 644 - 650
Role of Hydrogen in the Process of Sintering of Titanium Powders D. H. SavvakinM. M. HumenyakO. H. Molyar OriginalPaper 17 May 2012 Pages: 651 - 661
Influence of the components of microstructure on the static crack resistance of 13KHMF steel I. R. Dzioba OriginalPaper 18 May 2012 Pages: 662 - 669
Influence of the Phase-Structural State of the Surface Layers on the Mechanical Properties of VT1-0 Titanium Alloy A. T. PichuhinO. I. Yas’kivI. M. Pohrelyuk OriginalPaper 17 May 2012 Pages: 670 - 676
Fatigue Strength Improvement of AISI E52100 Bearing Steel by Induction Heating and Repeated Quenching E. C. SantosK. KidaJ. Rozwadowska OriginalPaper 17 May 2012 Pages: 677 - 682
Determination of the rate of atmospheric corrosion of metal structures by the method of polarization resistance L. I. NyrkovaS. H. PolyakovN. O. Hapula OriginalPaper 18 May 2012 Pages: 683 - 688
Formation of the joint of dissimilar metals in the solid phase by the method of vacuum hot rolling B. V. Borts OriginalPaper 18 May 2012 Pages: 689 - 695
Electrochemical properties of welded joints of 17G1SU steel M. S. KhomaH. M. SysynM. Ya. Holovchuk OriginalPaper 18 May 2012 Pages: 696 - 702
Remote determination of mechanical parameters of thin flat inclusions of low contrast Ya. I. Kunets’V. V. MatusM. D. Hrylyts’kyi OriginalPaper 17 May 2012 Pages: 703 - 709
Influence of hydrogen sorption on the kinetics of phase decomposition of RFe2 intermetallic compounds A. H. Vasyl’ev OriginalPaper 18 May 2012 Pages: 710 - 716