Chemical, mechanical and microstructural characterization of low-oxygen containing silicon carbide fibers with ceramic coatings N. P. BansalY. L. Chen OriginalPaper Pages: 5277 - 5289
Relationship between strength and failure mode of ceramic multilayers B. F. SørensenS. Primdahl OriginalPaper Pages: 5291 - 5300
Microstructure evolution and grain growth in the sintering of 3Y–TZP ceramics J. LuoS. AdakR. Stevens OriginalPaper Pages: 5301 - 5309
On the failure of unidirectional carbon-epoxy composites Part I:The effect of fibre sizing upon filament fracture and damage evolution C. MarstonC. Galiotis OriginalPaper Pages: 5311 - 5325
Response surface study on production of explosively-welded aluminum-titanium laminates E. S. EgeO. T. InalC. A. Zimmerly OriginalPaper Pages: 5327 - 5338
Single crystal fibers of yttria-stabilized cubic zirconia with ternary oxide additions F. J. RitzertH. M. YunR. V. Miner OriginalPaper Pages: 5339 - 5349
Friction and plasticity effects in wedge splitting and cutting fracture tests J. G. Williams OriginalPaper Pages: 5351 - 5357
Successful synthesis of Hg0.80Re0.20Sr2Can−1CunO2n+2+δ (n = 1, 2) by the sealed quartz tube technique A. CallejaA. SinX. Obradors OriginalPaper Pages: 5359 - 5363
Fabrication of in situ TiC reinforced aluminum matrix composites Part I: Microstructural characterization X. C. Tong OriginalPaper Pages: 5365 - 5374
Filament fracture within glass fibre strands in hybrid fibre cement composites M. KakemiD. J. HannantM. Mulheron OriginalPaper Pages: 5375 - 5382
Influence of poly(acrylic acid) molar mass on the fracture properties of glass polyalkenoate cements S. GriffinR. Hill OriginalPaper Pages: 5383 - 5396
Chalcogenide glasses for optical brazing S. M. SongS. Y. ChoiY. J. Baik OriginalPaper Pages: 5397 - 5400
Radial GRIN glasses in Li2O-Na2O-Al2O3-TiO2-SiO2 systems N. SoodbiswasS. K. SarkarA. Basuray OriginalPaper Pages: 5401 - 5403
The L12 ↔ DO19 transformation in the intermetallic compound Fe3Ge Q. Z. ChenA. H. W. NganB. J. Duggan OriginalPaper Pages: 5405 - 5414
Failure modes of fibre reinforced composites: The effects of strain rate and fibre content O. I. OkoliG. F. Smith OriginalPaper Pages: 5415 - 5422
Characterization of the imidization process of Low K-fluorinated polymide film during thermal curing Y. K. LeeS. P. Murarka OriginalPaper Pages: 5423 - 5426
Test methodology for the thermal shock characterization of ceramics V. R. VedulaD. J. GreenA. E. Segall OriginalPaper Pages: 5427 - 5432
Calcium hydroxyapatites: evaluation of sorption properties for cadmium ions in aqueous solution S. MandjinyK. A. MatisD. Jones OriginalPaper Pages: 5433 - 5439
On the phase composition of polymethylsiloxane derived ceramics M. J. WildP. Buhler OriginalPaper Pages: 5441 - 5444
Fabrication and mechanical properties of glass fibre–carbon fibre polypropylene functionally gradient materials Jyongsik JangCholho Lee OriginalPaper Pages: 5445 - 5450
Effect of water removal on the textural properties of resorcinol/formaldehyde gels by azeotropic distillation N. JabeenALI Mardan OriginalPaper Pages: 5451 - 5453
A study of the mechanical properties of highly porous ceramics using acoustic emission J. AuéJ. T. M. de Hosson OriginalPaper Pages: 5455 - 5462
The effect of substrate surface nature on texture formation in nickel oxide F. CzerwinskiJ. A. Szpunar OriginalPaper Pages: 5463 - 5472
Toughening of epoxies through thermoplastic crack bridging B. J. CardwellA. F. Yee OriginalPaper Pages: 5473 - 5484