Abstract
Using temperature-modulated differential scanning calorimetry, the melting behaviour of poly(oxytetramethylene)-alt-(aromatic oligoamide) (POTM-alt-AOA) has been studied in comparison with that of polyoxytetramethylene glycohols (POTMGs). The apparent melting temperature of the block copolymers is found to be less than that of the corresponding POTMGs by approximately 30°C. The relaxation time of melting of a POTM segment has been estimated and compared with that of POTMG. The relaxation time of POTM-alt-AOA is slightly shorter than that of POTMG when the molar mass of the POTM segment is 2900; however, it is longer when the molar mass is 1400.
Similar content being viewed by others
References
M El Fray (2000) Designed Monomers Polym. 3 325 Occurrence Handle10.1163/156855500300160276 Occurrence Handle1:CAS:528:DC%2BD3cXosF2kurY%3D
JP Sheth J Xu GL Wilkes (2003) Polymer 44 743 Occurrence Handle10.1016/S0032-3861(02)00798-X Occurrence Handle1:CAS:528:DC%2BD38XpsFaqsrk%3D
EV Konyukhova AI Buzin YK Godovsky (2002) Thermochim. Acta 391 271 Occurrence Handle10.1016/S0040-6031(02)00189-2 Occurrence Handle1:CAS:528:DC%2BD38Xls12gs7k%3D
R Ukielski M Piątek (2004) J. Therm. Anal. Cal. 77 259 Occurrence Handle10.1023/B:JTAN.0000033211.83644.11 Occurrence Handle1:CAS:528:DC%2BD2cXlt1ynsL8%3D
M Tsuchiya M Ishii T Kojima Y Oohira (1999) J. Therm. Anal. Cal. 56 1163 Occurrence Handle10.1023/A:1010113230133 Occurrence Handle1:CAS:528:DyaK1MXnt1Wnurc%3D
K Tago M Tsuchiya Y Gondo K Ishimaru T Kojima (2000) J. Appl. Polym. Sci. 77 1538 Occurrence Handle10.1002/1097-4628(20000815)77:7<1538::AID-APP15>3.0.CO;2-J Occurrence Handle1:CAS:528:DC%2BD3cXkt12lt7Y%3D
M Tsuchiya T Kojima (2003) J. Therm. Anal. Cal. 72 654 Occurrence Handle10.1023/A:1024598221061
M Tsuchiya T Kojima (2005) J. Therm. Anal. Cal. 80 159 Occurrence Handle10.1007/s10973-005-0629-2 Occurrence Handle1:CAS:528:DC%2BD2MXktl2ks74%3D
W Miyano E Inoue M Tsuchiya K Ishimaru T Kojima (2001) J. Therm. Anal. Cal. 64 459 Occurrence Handle10.1023/A:1011553826342 Occurrence Handle1:CAS:528:DC%2BD3MXkslWlt7s%3D
MCE Niesten J Feijen RJ Gaymans (2001) Polymer 42 6199 Occurrence Handle10.1016/S0032-3861(01)00088-X Occurrence Handle1:CAS:528:DC%2BD3MXisF2nsL4%3D
MCE Niesten JW ten Brinke TJ Gaymans (2001) Polymer 41 1461 Occurrence Handle10.1016/S0032-3861(00)00430-4
MCEJ Niesten J Feijen RJ Gaymans (2000) Polymer 41 8487 Occurrence Handle10.1016/S0032-3861(00)00252-4 Occurrence Handle1:CAS:528:DC%2BD3cXlt1Kitr8%3D
A Toda C Tomita M Hikosaka Y Saruyama (1998) Polymer 39 5039
JEK Schawe (1995) Thermochim. Acta 260 1 Occurrence Handle1:CAS:528:DyaK2MXnvFWltL4%3D Occurrence Handle10.1016/0040-6031(95)90466-2
B Wunderlich Y Jin A Boller (1994) Thermochim. Acta 238 277 Occurrence Handle10.1016/S0040-6031(94)85214-6 Occurrence Handle1:CAS:528:DyaK2cXls1Gjt7g%3D
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Tsuchiya, M., Inomura, A. & Kojima, T. Melting behavior of poly(oxytetramethylene)-alt-(aromatic oligoamide) block copolymers. J Therm Anal Calorim 88, 471–475 (2007). https://doi.org/10.1007/s10973-006-8089-x
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s10973-006-8089-x