Abstract
Pollution and climate change issues are calling for advanced techniques of pollutant sequestration to decrease toxicity, of coral and costal remediation, and of carbon sequestration to decrease atmospheric CO2 levels. For that, calcareous deposition appears as an overlooked, but potentially efficient technique. The calcareous deposit is a well-known precipitation by-product of cathodic protection in seawater. The deposit is made of a mixture of CaCO3 and Mg(OH)2. A calcareous deposit is formed electrochemically when a metal connected to an electrical power source is immersed in seawater. So far, electrochemical calcareous deposition has seldomly found applications, except for speedup of coral growth, prevention of shore erosion, reinforcement of artificial marine structures and remediation of polluted seawater. Here, we review the principles and mechanisms of electrochemical calcareous deposition. The growth, composition and mechanical properties of calcareous deposits are controlled by several factors such as 1) the impact of electrochemical parameters on the Ca/Mg ratio. For instance, CaCO3 formation is favoured at low cathodic potentials and low currents, whereas Mg(OH)2 precipitates preferentially at high cathodic potentials and high applied current; 2) the nature of the metallic electrode: although lime could be deposited onto any metallic surface at a fixed potential, electrochemical reactions and deposit composition are controlled by the metal nature. Moreover, the state of the electrode surface, e.g. with the presence of oxides or biofilms, modifies the kinetics of deposit formation; and 3) electrolyte composition, pH, temperature and stirring. For instance, in seawater, Ca2+ and Mg2+ concentrations control the allotropic variety of CaCO3 formed, e.g. Mg2+ inhibits the formation of calcite and vaterite. Hydrodynamic conditions near the electrode also influence the deposit composition since conditions regulate the mass transport at the electrode–solution interface. Below 10 °C, aragonite is not formed and the deposit stays thin. In the first stage of the deposit formation, an Mg-based compound is formed, followed by the growth of a Ca-based compound with time.
Similar content being viewed by others
References
Akamine K, Kashiki I (2002) Corrosion protection of steel by calcareous electrodeposition in seawater part 1: mechanism of electrodeposition. Zair to Kankyo 51:496–501
Akamine K, Kashiki I (2003) Corrosion protection of steel by calcareous electrodeposition in seawater part 2: mechanism of growth. Zair to Kankyo 52:401–407
Al-Hazmi F, Umar A, Dar GN et al (2012) Microwave assisted rapid growth of Mg(OH)2 nanosheet networks for ethanol chemical sensor application. J Alloys Compd 519:4–8. https://doi.org/10.1016/j.jallcom.2011.09.089
ASTM International (1998) Standard for the preparation of substitute ocean water
Barchiche C (2004) Caractérisation et cinétique de formation des dépôts calcomagnésiens sur acier en eau de mer artificielle/Characterization and formation kinetics of calcareousdeposits on steel in artificialseawater. Ph.D Dissertation, University of La Rochelle, France
Barchiche C, Deslouis C, Festy D et al (2003) Characterization of calcareous deposits in artificial seawater by impedance techniques: III. Deposit of CaCO3 in the presence of Mg(II). Electrochim Acta 48:1645–1654. https://doi.org/10.1016/S0013-4686(03)00075-6
Barchiche C, Deslouis C, Gil O et al (2004) Characterisation of calcareous deposits by electrochemical methods: role of sulphates, calcium concentration and temperature. Electrochim Acta 49:2833–2839. https://doi.org/10.1016/j.electacta.2004.01.067
Barchiche C, Deslouis C, Gil O et al (2009) Role of sulphate ions on the formation of calcareous deposits on steel in artificial seawater; the formation of Green Rust compounds during cathodic protection. Electrochim Acta 54:3580–3588. https://doi.org/10.1016/j.electacta.2009.01.023
Beaunier L, Gabrielli C, Poindessous G et al (2001) Investigation of electrochemical calcareous scaling: nuclei counting and morphology. J Electroanal Chem 501:41–53. https://doi.org/10.1016/S0022-0728(00)00481-2
Braterman PS, Cygan RT (2006) Vibrational spectroscopy of brucite: a molecular simulation investigation. Am Miner 91:1188–1196. https://doi.org/10.2138/am.2006.2094
Brindley GW, Kao CC (1984) Structural and IR relations among brucite-like divalent metal hydroxides. Phys Chem Miner 10:187–191. https://doi.org/10.1007/BF00311476
Carré C, Gunkel-Grillon P, Serres A et al (2017) Calcareous electrochemical precipitation, a new method to trap nickel in seawater. Environ Chem Lett 15:151–156. https://doi.org/10.1007/s10311-016-0602-2
Carré C, Gunkel-Grillon P, Serres A et al (2019) Laboratory and in situ investigations for trapping Pb and Ni with an unusual electrochemical device, the calcareous deposit in seawater. Sci Rep 9:3–10. https://doi.org/10.1038/s41598-019-40307-0
Caspi EN, Pokroy B, Lee PL et al (2005) On the structure of aragonite. Acta Crystallogr Sect B Struct Sci 61:129–132. https://doi.org/10.1107/S0108768105005240
Ce N, Paul S (2017) The effect of temperature and local pH on calcareous deposit formation in damaged thermal pray aluminum (TSA) coatings and its implication on corrosion mitigation of offshore steel structures. Coatings 7:52. https://doi.org/10.3390/coatings7040052
Cox GC (1940) Anticorrosive and antifouling coating and method of application. United States Patent
Cox GC (1947) Rust-inhibiting coating composition. United States Patent
Davy H (1840) Protection of the copper sheating of ships, by electrical combinations. In: Davy J (ed) The collected works of Sir Humphry Davy—volume VI—miscellaneous papers and researches. Smith, Eld, London, pp 273–285
Deslouis C, Frateur I, Maurin G, Tribollet B (1997) Interfacial pH measurement during the reduction of dissolved oxygen in a submerged impinging jet cell. J Appl Electrochem 27:482–492. https://doi.org/10.1023/A:1018430224622
Deslouis C, Festy D, Gil O et al (1998) Characterization of calcareous deposits in artificial seawater by impedance techniques: I. Deposit of CaCO3 without Mg(OH)2. Electrochim Acta 43:1891–1901. https://doi.org/10.1016/S0013-4686(97)00303-4
Deslouis C, Festy D, Gil O et al (2000) Characterization of calcareous deposits in artificial seawater by impedances techniques: II. Deposit of Mg(OH)2 without CaCO3. Electrochim Acta 45:1837–1845. https://doi.org/10.1016/S0013-4686(99)00403-X
Devos O, Jakab S, Gabrielli C et al (2009) Nucleation-growth process of scale electrodeposition—influence of the magnesium ions. J Cryst Growth 311:4334–4342. https://doi.org/10.1016/j.jcrysgro.2009.07.021
Dexter SC, Lin S-H (1992a) Effect of marine biofilms on cathodic protection. Int Biodeterior Biodegrad 29:231–249. https://doi.org/10.1016/0964-8305(92)90046-Q
Dexter SC, Lin SH (1992b) Calculation of seawater pH at polarized metal-surfaces in the presence of surface-films. Corrosion 48:50–60
Eashwar M, Subramanian G, Palanichamy S et al (2009) Cathodic behaviour of stainless steel in coastal Indian seawater: calcareous deposits overwhelm biofilms. Biofouling 25:191–201. https://doi.org/10.1080/08927010802670267
Edyvean RGJ, Maines AD, Hutchinson CJ et al (1992) Interactions between cathodic protection and bacterial settlement on steel in seawater. Int Biodeterior Biodegrad 29:251–271. https://doi.org/10.1016/0964-8305(92)90047-R
Eickhoff AJ, Shaw WE (1948) Principles of protecting metals with organic coatings. Corrosion 4:463–475
Elfil H, Roques H, Roquesb H (2001) Role of hydrate phases of calcium carbonate on the scaling phenomenon. Desalination 137:177–186. https://doi.org/10.1016/S0011-9164(01)00216-8
Euvrard M, Membrey F, Filiatre C et al (2006) Kinetic study of the electrocrystallization of calcium carbonate on metallic substrates. J Cryst Growth 291:428–435. https://doi.org/10.1016/j.jcrysgro.2006.03.025
Festy D, Vittonato J, Hesjevik SM, Merchant I (2011) ICP-DATA: in situ data collection for cathodic protection design. In: NACE corrosion
Gabrielli C, Maurin G, Perrot H et al (2002) Investigation of electrochemical calcareous scaling: potentiostatic current– and mass–time transients. J Electroanal Chem 538–539:133–143. https://doi.org/10.1016/S0022-0728(02)01044-6
Gabrielli C, Jaouhari R, Joiret S et al (2003) Study of the electrochemical deposition of CaCO3 by in situ Raman spectroscopy. J Electrochem Soc 150:C478. https://doi.org/10.1149/1.1579482
Gil O, Refait P, Memet JB, Seguy L (2000) Étude des dépôts calcomagnésiens formés sur acier lors de la protection cathodique: dépôts naturels et dépôts préparés en laboratoire/Study of calcareousdepositsformed on steelduringcathodic protection: naturaldeposits and depositsprepared in lab. J Eur d’hydrol 31:167–182
Godart C, Dagbert C (2004) Impact de l’environnment marin sur la formation du dépôt calco-magnésien: rôle de la matière organique/Marine environment influence on calcareous deposit formation: role of organic matter. Matér Tech 92:27–32
Goreau TJ (2012) Marine electrolysis for building materials and environmental restoration. In: Kleperis J, Linkov V (eds) Electrolysis. InTech, Croatia, pp 273–290
Grazulis S, Chateigner D, Downs RT et al (2009) Crystallography open database—an open-access collection of crystal structures. J Appl Crystallogr 42:726–729. https://doi.org/10.1107/S0021889809016690
Hartt WH, Culberson CH, Smith SW (1984) Calcareous deposits on metal surfaces in seawater—a critical review. Corrosion 40:609–618
Hernandez G, Hartt WH, Videla HA (1994) Marine biofilms and their influence on cathodic protection: a literature survey. Corros Rev 12:29–40. https://doi.org/10.1515/CORRREV.1994.12.1-2.29
Hilbertz WH (1979) Electrodeposition of minerals in sea water: experiments and applications. IEEE J Ocean Eng 4:94–113. https://doi.org/10.1109/JOE.1979.1145428
Humble RA (1948) Cathodic protection of steel in seawater with magnesium anodes. Corrosion 4:358–370
Humble HA (1949) The cathodic protection of steel piling in seawater. Corrosion 5:292–302. https://doi.org/10.1017/CBO9781107415324.004
International Centre for Diffraction Data (ICDD) (1999) Powder diffraction files (PDF)
Karoui H, Riffault B, Jeannin M et al (2013) Electrochemical scaling of stainless steel in artificial seawater: role of experimental conditions on CaCO3 and Mg(OH)2 formation. Desalination 311:234–240. https://doi.org/10.1016/j.desal.2012.07.011
Kitano Y, Hood DW (1965) The influence of organic material on the polymorphic crystallization of calcium carbonate. Geochim Cosmochim Acta 29:29–41. https://doi.org/10.1016/0016-7037(65)90075-X
Langumier M, Lanneluc I, Sabot R et al (2011) Quelles sont les bactéries présentes dans les biofilms formés sur acier en milieu marin?/Which bacteria are present in the biofilms developed on carbon steel in marine environment? Matér Tech 99:591–603. https://doi.org/10.1051/mattech/2011114
Lewandowski Z, Beyenal H (2014) Fundamentals of biofilm research, 2nd edn. Taylor and CRC Predd, London
Li C, Du M, Qiu J et al (2014) Influence of temperature on the protectiveness and morphological characteristics of calcareous deposits polarized by galvanostatic mode. Acta Metall Sin 27:131–139. https://doi.org/10.1007/s40195-013-0010-6
Lin SH, Dexter SC (1988) Effects of temperature and magnesium ions on calcareous deposition. Corrosion 44:615–622. https://doi.org/10.5006/1.3584974
Loste E, Wilson RM, Seshadri R, Meldrum FC (2003) The role of magnesium in stabilising amorphous calcium carbonate and controlling calcite morphologies. J Cryst Growth 254:206–218. https://doi.org/10.1016/S0022-0248(03)01153-9
Luo JS, Lee RU, Chen TY et al (1991) Formation of calcareous deposits under different modes of cathodic polarization. Corrosion 47:189–196
Markgraf SA, Reeder RJ (1985) High-temperature structure refinements of calcite and magnesite. Am Miner 70:590–600
Meijer JAM, Van Rosmalen GM (1984) Solubilities and super saturations of calcium sulfate and its hydrates in seawater. Desalination 51:255–305. https://doi.org/10.1016/0011-9164(84)87002-2
Millero FJ, Pierrot D (1998) A chemical equilibrium model for natural waters. Aquat Geochem 4:153–199. https://doi.org/10.1023/A:1009656023546
Möller H (2007) The influence of Mg2+ on the formation of calcareous deposits on freely corroding low carbon steel in seawater. Corros Sci 49:1992–2001. https://doi.org/10.1016/j.corsci.2006.10.011
Morse JW, Arvidson RS, Lüttge A (2007) Calcium carbonate formation and dissolution. Chem Rev 107:342–381. https://doi.org/10.1021/cr050358j
Munksgaard NC, Wurster CM, Bass A, Zagorskis I, Bird MI (2012) First continuous shipboard δ18O and δD measurements in sea water by diffusion sampling—cavity ring-down spectrometry. Environ Chem Lett 10:301–307. https://doi.org/10.1007/s10311-012-0371-5
Nancollas G, Kazmierczak T, Schuttringer E (1981) A controlled composition study of calcium carbonate crystal growth: the influence of scale inhibitors. Corrosion 37:76–81
Neville A, Morizot AP (2002) Calcareous scales formed by cathodic protection—an assessment of characteristics and kinetics. J Cryst Growth 243:490–502. https://doi.org/10.1016/s0022-0248(02)01532-4
Nguyen Dang D, Gascoin S, Zanibellato A et al (2017) Role of brucite dissolution in calcium carbonate precipitation from artificial and natural seawaters. Cryst Growth Des 17:1502–1513. https://doi.org/10.1021/acs.cgd.6b01305
Perry RH, Green DW, Maloney JO (1997) Perry’s chemical engineers’ handbook seventh. McGraw-Hill, New York
Philipponeau G (1982) Influence de divers facteurs sur les comportements électrochimique et mécanique d’aciers faiblement alliés, polarisés cathodiquement ou non en milieu de type marin/Influence of various factors on the electrochemical and mechanical behaviors of low-alloy. Ph.D. Dissertation, Centre de Recherche de l’Ecole Centrale des Arts et Manufactures de Paris, France
Pytkowicz RM, Kester DR (1969) Harned’s rule behavior of NaCl–Na2SO4 solutions explained by an ion association model. Am J Sci 267:217–229
Rousseau C, Baraud F, Leleyter L et al (2010) Calcareous deposit formed under cathodic protection in the presence of natural marine sediments: a 12 month experiment. Corros Sci 52:2206–2218. https://doi.org/10.1016/j.corsci.2010.02.047
Salvago G, Maffi S, Benedetti A, Magagnin L (2004) Coating electroaccretion on galvanized iron and aluminum in seawater. Electrochim Acta 50:169–178. https://doi.org/10.1016/j.electacta.2004.07.028
Sarkar A, Mahapatra S (2010) Synthesis of all crystalline phases of anhydrous calcium carbonate. Cryst Growth Des 10:2129–2135. https://doi.org/10.1021/cg9012813
Stumm W, Morgan JJ (1996) Aquatic chemistry—chemical equilibria and rates in natural waters, 3rd edn. Wiley, Hoboken
Sung-Tsuen L, Nancollas GH (1973) The crystallization of magnesium hydroxide. Desalination 12:75–84. https://doi.org/10.1016/S0011-9164(00)80176-9
Tlili MM, Ben Amor M, Gabrielli C et al (2002) Characterization of CaCO3 hydrates by micro-Raman spectroscopy. J Raman Spectrosc 33:10–16. https://doi.org/10.1002/jrs.806
Tlili MM, Ben Amor M, Gabrielli C et al (2003) Influence of the interfacial pH on electrochemical CaCO3 precipitation. J Electrochem Soc 150:C765. https://doi.org/10.1149/1.1613294
Touzain S (1996) Etude de la structure des dépôts calcomagnésiens sur acier en eau de mer artificielle/Study of calcareousdeposit structure on steel in artificialseawater. Ph.D. Dissertation, La Rochelle, France
Tu K, Cottis RA (2009) Controlling the components of calcareous deposit to protect steel structures from ALWC with DC and pulse current. Corrosion 2009:1–16
Vedrenne B, Scharr P (2005) Procédé pour la formation de ciment ou béton par électrolyse/Method for forming cement or concrete by electrolysis
von Baeckmann W, Schwenk W, Prinz W (1997) Handbook of cathodic corrosion protection. Elsevier Science, Amsterdam
Wolfson SL, Hartt WH (1981) An initial investigation of calcareous deposits upon cathodic steel surfaces in sea water. Corrosion 37:70–76
Yan J-F, White RE, Griffin RB (1993) Parametric studies of the formation of calcareous deposits on cathodically protected steel in seawater. J Electrochem Soc 140:1275–1280. https://doi.org/10.1149/1.2220970
Zamanzade M, Shahrabi T, Yazdian A (2007) Improvement of corrosion protection properties of calcareous deposits on carbon steel by pulse cathodic protection in artificial sea water. Anti-Corros Methods Mater 54:74–81. https://doi.org/10.1108/00035590710733566
Zanibellato A (2016) Synthèse et études physico-chimiques d’un agglomérat calcomagnésien formé sur acier en milieu marin: un éco-matériau pour la protection du littoral/Synthesis and physico-chemical studies of a calcareous agglomerate formed on steel in marine environment. Ph.D. Dissertation, La Rochelle, France
Author information
Authors and Affiliations
Corresponding author
Additional information
Publisher's Note
Springer Nature remains neutral with regard to jurisdictional claims in published maps and institutional affiliations.
Rights and permissions
About this article
Cite this article
Carré, C., Zanibellato, A., Jeannin, M. et al. Electrochemical calcareous deposition in seawater. A review. Environ Chem Lett 18, 1193–1208 (2020). https://doi.org/10.1007/s10311-020-01002-z
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s10311-020-01002-z