Abstract
Wood specimens were prepared in a swollen state using solvent exchange (PS) treatment. The swollen wood specimens were acetylated using acetic anhydride by heating at 80–120°C. At the beginning of heating, the weight percent gain (WPG) of PS-treated wood was greater than that of conventionally acetylated wood. This acceleration effect of the PS treatment was explained by the introduction of treating reagent into the wood polymers where the intermolecular hydrogen bonds were previously broken. On the other hand, the PS treatment had no influence on the final WPG and moisture sorption characteristics of acetylated wood. This indicated that the intrinsic reactivity of wood constituents was unaffected by the PS treatment. The acetylation of PS-treated wood produced greater bulking and slightly higher dimensional stability than that in the case of conventional acetylation at the same WPG. It was speculated that the expansion of cell lumina due to the PS treatment resulted in greater bulking on acetylation and lesser swelling of acetylated wood with moisture sorption.
Similar content being viewed by others
References
Hill CAS, Ormondroyd GA (2004) Dimensional changes in Corsican pine (Pinus nigra Arnold) modified with acetic anhydride measured using a helium pycnometer. Holzforschung 58(5):544–547
Hill CAS, Papadopoulos AN, Payne D (2004) Chemical modification employed as a means of probing the cell-wall micropore of pine sapwood. Wood Sci Technol 37(6):475–488
Minato K, Ito Y (2004) Analysis of the factors influencing the acetylation rate of wood. J Wood Sci 50:519–523
Minato K, Ogura K (2003) Dependence of reaction kinetics and physical and mechanical properties on the reaction systems of acetylation I: reaction kinetic aspects. J Wood Sci 49:418–422
Obataya E, Gril J (2005) Swelling of acetylated wood I: swelling in organic liquids. J Wood Sci 51:124–129
Obataya E, Ono T, Norimoto M (2000) Vibrational properties of wood along the grain. J Mater Sci 35 (12):2993–3001
Rowell RM (1982) Distribution of acetyl groups in southern pine reacted with acetic anhydride. Wood Sci 15(2):172–182
Rowell RM (1991) Chemical modification of wood. In: Wood and cellulosic chemistry. Marcel Dekker, New York
Rowell RM, Ellis WD (1978) Determination of the dimensional stabilization of wood using the water soak method. Wood Fiber Sci 10:104–111
Rowell RM, Simonsen R, Hess S, Plackett DV, Cronshaw D, Dunningham E (1994) Acetyl distribution in acetylated whole wood and reactivity of isolated cell wall components to acetic anhydride. Wood Fiber Sci 26(1):11–18
Skaar C (1988) Wood–water relations. Springer, Berlin Heidelberg New York
Stamm AJ, Tarkow H (1947) Dimensional stabilization of wood. J Coll Chem 51:493–505
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Obataya, E., Minato, K. Effects of previous solvent exchange on acetylation of wood. Wood Sci Technol 41, 351–360 (2007). https://doi.org/10.1007/s00226-006-0111-8
Received:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s00226-006-0111-8