Abstract
On copper doped ZnO-crystals the angular, doping and temperature dependence of the ESR line width has been investigated. The measurements on different conventionally and radiochemically doped ZnO-crystals show the strong influence of the perfectness of the crystals on the line width. By the measured temperature dependence of the line width is deduced, that the spin-lattice relaxation mechanism between 7 and 17 °K is a Raman process.
Similar content being viewed by others
Author information
Authors and Affiliations
Additional information
Den Herren Prof. Dr. E. Mollwo, G. Müller und Prof. Dr. G. Heiland danken wir herzlich für die zur Verfügung gestellten ZnO-Einkristalle, Dr. K.-H. Franke und M. Gafron für die Bereitstellung der radiochemisch dotierten ZnO-Einkristalle. Für die Mittel zur Beschaffung der verwendeten ESR-Anlage sind wir der Deutschen Forschungsgemeinschaft zu Dank verpflichtet.
Rights and permissions
About this article
Cite this article
Broser, I., Schulz, M. Untersuchung der Breite der ESR-Signale von Cu2+ in ZnO-Kristallen. Z. Physik 254, 35–45 (1972). https://doi.org/10.1007/BF01379688
Received:
Issue Date:
DOI: https://doi.org/10.1007/BF01379688