Abstract
Castable machinable glass-ceramics have been widely considered as aesthetic materials for dental restoration. In order to extend their applications to bridge-work fabrication, it is necessary to increase their fracture strength and fracture toughness. The effects of ziconia and alumina additions on the properties of glass-ceramics, especially on the mechanical properties were studied. It was found that appropriate addition of alumina increases the bending strength due to aluminium strengthening the glass-ceramic by means of incorporation into the glass network. However, additions of ziconia fail to show promising results on the mechanical property. The evolution of recrystallization and the associated microstructure were also studied and are discussed.
Similar content being viewed by others
References
D. G. Grossman and H. Walters, J. Dent. Res. 63 (1984) 234.
S. F. Hulbert, L. L. Hench, K. Forbes, and L. S. Brwman, in “Ceramic in Surgery”, edited by P. Vincenzini (Elsevier Science, New York, 1983) p. 3.
W. J. McLean, Brit. Dent. J., 164 (1988) 1887.
W. T. MacCulloch, ibid.— 124 (1968) 361.
L. L. Hench, et al. J. Dent. Res. 50 (1971) 133.
D. J. Adair, US Pat. 4431420, 14 February 1984, US, Patent Office, Washington, D. C.
D. G. Grossman, US Pat. 3839055, 1 October, 1974, US, Patent Office, Washington, D. C.
Idem, J. Can. Ceram. Soc. 55 (1972) 446.
S. F. Rosenstiel, and S. S. Porter, J. Pros. Dent., 62 (1989) 529.
D. J. Green, R. H. J. Hannind, and M. V. Swain, in “Transformation Toughening of Ceramics” (CRC Press, Florida, 1989) Ch. 3.
J. G. Duh, H. T. Dai and B. S. Chiou, J. Am. Ceram. Soc. 71 (1988) 813.
“Installation Operation and Service Manual of DICOR”, Dentsply International and Corning Glass Works. York, PA, USA (1987).
F. Seifert and W. Schreyer, Am. Mineral 50 (1965) 1114.
J. M. Tzeng, MS thesis, National Tsing Hua University, Hsinchu, Taiwan (1990)
F. de Mestral and R. A. L. Drew, J. Eur. Ceram. Soc. 5 (1989) 47.
J. S. Olcott and S. D. Stookey, US Pat. 2998675, 5 September, 1961, US Patent Office Washington, D. C.
C. K. Chyung, F. J. Beall and D. G. Grossman, in “Electron Microscopy and Structure of Materials”, edited by G. Thomas (University California Press, Berkeley, 1971) pp. 1167–94.
M. B. Volf, in “Chemical Approach to Glass” (Elsevier, Amsterdam, 1984) Ch. 14.
W. D. Kingery, H. K. Bowen, and D. R. Uhlmann, in “Introduction to Ceramics”, 2nd Edn (Wiley, New York, 1976) Ch. 3.
R. D. Shannon and C. T. Prewitt, Acta Crystallog. B25 (1969) 925.
A. A. Griffith, Phil. Trans. R. Soc. a221 (1924) 163.
R. E. Reed-Hill and R. Abbaschian, in “Physical Metallurgy Principles”, 3rd Edn (PWS-KENT, Boston, MA, 1992) Ch. 22.
M. B. Volt, in “Chemical Approach to Glass” (Elsevier, Amsterdam. 1984) Ch. 16.
M. Nogami and K. Nagaska, J. Non-Cryst. Solid, 100 (1988) 298.
J. R. Kelly, S. D. Campbell and H. K. Bowen, J. Pros. Dent. 62 (1989) 536.
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Tzeng, J.M., Duh, J.G., Chung, K.H. et al. Al2O3-and ZrO2-modified dental glass ceramics. JOURNAL OF MATERIALS SCIENCE 28, 6127–6135 (1993). https://doi.org/10.1007/BF00365033
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/BF00365033