The Tensile Fracture of Ag-Containing Al-Li-Cu-Mg-Zr Alloys

  • X. J. Jiang
  • Y. Y. Li
  • C. X. Shi
Part of the An International Cryogenic Materials Conference Publication book series (ACRE, volume 40)

Abstract

The tensile properties and fracture characteristics of two kinds of Ag-containing Al-Li-Cu-Mg-Zr alloys with different aging conditions have been studied from 290 to 77 K. The results show that the tensile strength and ductility of the alloys improved significantly with a decrease in test temperature from 153 to 77 K, except for the elongation of some alloys in certain aging conditions. Planar slip behavior is the predominant deformation mode for the natural-, under-, and peak-aged samples when tested at room temperature, but the slip distribution is fairly homogeneous as the test temperature is reduced to 77 K. The different modes of tensile fracture are closely associated with the aging time and test temperatures. The improvement in cryogenic ductility of the alloys can be attributed to an increase in deformation homogeneity. The tensile fracture behavior of the alloys at ambient and cryogenic temperatures are discussed.

Keywords

Test Temperature Slip Band Naturally Aged Tensile Fracture Cryogenic Temperature 
These keywords were added by machine and not by the authors. This process is experimental and the keywords may be updated as the learning algorithm improves.

Preview

Unable to display preview. Download preview PDF.

Unable to display preview. Download preview PDF.

References

  1. 1.
    J. Glazer, S. L. Verzasconi, R. R. Sawtell, and J. W. Morris, Jr., Mechanical behavior of aluminum-lithium alloys at cryogenic temperatures, Metall. Trans. A 18A: 1695 (1987).Google Scholar
  2. 2.
    Y. B. Xu, L. Wang, Y. Zhang, Z. G. Wang, and Z. Q. Hu, Metall. Trans. A 22A: 723 (1991).CrossRefGoogle Scholar
  3. 3.
    R. C. Dorward, Cryogenic toughness of Al-Cu-Li alloy AA 2090, Ser. Metall. 21: 1379 (1986).CrossRefGoogle Scholar
  4. 4.
    H. J. Roven, E. A. Starke, Jr., O. Sedahl, and J. Hjelen, Effects of texture on delamination behavior of 8090-type Al-Li alloy at cryogenic and room temperature, Scr. Metall. 24: 421 (1990).CrossRefGoogle Scholar
  5. 5.
    K. Welpmann, Y.T. Lee, and M. Peters, Low temperature deformation phenomena of the Al-Li alloy 8090, Mater. Sci. Eng. Al29: 21 (1990).Google Scholar
  6. 6.
    J. W. Morris, Jr. and J. Glazer, Mechanical behavior of high-strength aluminum alloys at cryogenic temperatures, p. 713 in: “Cryogenic Materials ‘88,” R. P. Reed, Z. S. Xing, and E. W. Collings, eds., International Cryogenic Materials Conference, Boulder, Colorado (1988).Google Scholar
  7. 7.
    X. J. Jiang, Microstructure and tensile fracture mechanisms of Al-Li alloys containing Zn, Ag or Sc, Ph.D. Dissertation, Institute of Metal Research, Academia Sinica, Shenyang, China (1993).Google Scholar
  8. 8.
    X. J. Jiang, Q. H. Gui, Y. Y. Li, L. M. Ma, G. J. Liang, and C. X. Shi, Effects of minor additions on precipitation and properties of Al-Li-Cu-Mg-Zr alloy, Scr. Metall. Mater. 29: 211 (1993).CrossRefGoogle Scholar
  9. 9.
    X. J. Jiang and Y. Y. Li, Al-Li-Cu-Mg-Zr base alloys containing silver and/or scandium, Chinese patent application number 92106154.4 (April 27, 1992 ).Google Scholar
  10. 10.
    D. Dew-Hughes, E. Creed, and W. S. Miller, Grain boundary failure in an Al-Li alloy, Mater. Sci. Technol. 4: 106 (1988).CrossRefGoogle Scholar

Copyright information

© Springer Science+Business Media New York 1994

Authors and Affiliations

  • X. J. Jiang
    • 1
  • Y. Y. Li
    • 1
  • C. X. Shi
    • 1
  1. 1.Institute of Metal ResearchAcademia SinicaShenyangChina

Personalised recommendations