Catalyst Degradation Mechanisms in PEM and Direct Methanol Fuel Cells

  • Conference paper
Mini-Micro Fuel Cells

While much attention has been given to optimizing initial fuel cell performance, only recent research has focused on the various materials degradation mechanisms observed over the life-time of fuel cells under real-life operating conditions. This presentation will focus on fuel cell durability constraints produced by platinum sintering/dissolution, carbon-support oxidation, and membrane chemical and mechanical degradations.

Over the past 10 years, extensive R&D efforts were directed towards optimizing catalysts, membranes, and gas diffusion layers (GDL) as well as combining them into improved membrane electrode assemblies (MEAs), leading to significant improvements in initial performance of H2/air-fed proton exchange membrane fuel cells (PEMFCs) and methanol/air-fed direct methanol fuel cells (DMFCs). While the required performance targets have not yet been met, current PEMFC and DMFC performance are close to meeting entry-level applications and many prototypes have been developed for field testing. This partially shifted the R&D focus from performance optimization to more closely examining materials degradation phenomena which limit fuel cell durability under real-life testing conditions.

The predominant degradation mechanisms are sintering/dissolution of platinum-based cathode catalysts under highly dynamic operating conditions, dissolution of ruthenium from DMFC anode catalysts, the oxidation of carbon-supports of the cathode catalyst during fuel cell startup and shutdown, and the formation of pinholes in proton exchange membranes if subjected to extensive local relative humidity cycling. These various mechanisms and their impact of fuel cell durability will be discussed in the following.

This is a preview of subscription content, log in via an institution to check access.

Access this chapter

Chapter
USD 29.95
Price excludes VAT (USA)
  • Available as PDF
  • Read on any device
  • Instant download
  • Own it forever
eBook
USD 169.00
Price excludes VAT (USA)
  • Available as PDF
  • Read on any device
  • Instant download
  • Own it forever
Softcover Book
USD 219.99
Price excludes VAT (USA)
  • Compact, lightweight edition
  • Dispatched in 3 to 5 business days
  • Free shipping worldwide - see info
Hardcover Book
USD 219.99
Price excludes VAT (USA)
  • Durable hardcover edition
  • Dispatched in 3 to 5 business days
  • Free shipping worldwide - see info

Tax calculation will be finalised at checkout

Purchases are for personal use only

Institutional subscriptions

Preview

Unable to display preview. Download preview PDF.

Unable to display preview. Download preview PDF.

References

  1. H.A. Gasteiger, S.S. Kocha, B. Sompalli, and F.T. Wagner, Activity Benchmarks and Requirements for Pt, Pt-Alloy, and Non-Pt Oxygen Reduction Catalysts for PEMFCs, Appl. Catal. B 56, 9 (2005).

    Article  Google Scholar 

  2. P. Piela and P. Zelenay, Researchers Redefine The DMFC Roadmap, The Fuel Cell Review Aug./Sept., 17 (2004).

    Google Scholar 

  3. J. Müller, G. Frank, K. Colbow, and D. Wilkinson, “Transport/Kinetic Limitations and Efficiency Losses”, in: Handbook of Fuel Cells: Fundamentals, Technology, and Applications, edited by W. Vielstich, A. Lamm, and H.A. Gasteiger (Wiley, Chichester, UK, 2003), vol. 3, pp. 847-855.

    Google Scholar 

  4. P.J. Ferreira, G.J. la O’, Y. Shao-Horn, D. Morgan, R. Makharia, S.S. Kocha, and H.A. Gasteiger, Instability of Pt/C Electrocatalysts in Proton Exchange Membrane Fuel Cells - A Mechanistic Investigation, J. Electrochem. Soc. 152, A2256 (2005).

    Article  Google Scholar 

  5. P. Piela, C. Eickes, E. Brosha, F. Garzon, and P. Zelenay, Ruthenium Crossover in Direct Methanol Fuel Cell with Pt-Ru Black Anode, J. Electrochem. Soc. 151, A2053 (2004).

    Article  Google Scholar 

  6. C.A. Reiser, L. Bregoli, T.W. Patterson, J.S. Yi, J.D. Yang, M.L. Perry, and T.D. Jarvi,  A Reverse-Current Decay Mechanism for Fuel Cells, Electrochem. Solid State Lett. 8, A273 (2005).

    Article  Google Scholar 

  7. M.F. Mathias, R. Makharia, H.A. Gasteiger, J.J. Conley, T.J. Fuller, C.J. Gittleman, S.S. Kocha, D.P. Miller, C.K. Mittelsteadt, T. Xie, S.G. Yan, and P.T. Yu, Two Fuel Cell Cars In Every Garage? Interface (The Electrochemical Society, 2005), 14, pp. 24-35.

    Google Scholar 

  8. T. Tada, “High Dispersion Catalysts Including Novel Carbon-Supports”, in: Handbook of Fuel Cell, edited by W. Vielstich, A. Lamm, and H.A. Gasteiger (Wiley, Chichester, UK, 2003), vol. 3, pp. 481-488.

    Google Scholar 

  9. H.A. Gasteiger, Y. Liu, D. Baker, and W. Gu, “Kinetics and Kinetically Limited Performance in PEMFCs and DEMFCs with State-of-the-Art Catalysts”, in this book.

    Google Scholar 

  10. K. Kinoshita, J.T. Lundquist, and P. Stonehart, Potential Cycling Effects on Platinum Electrocatalyst Surfaces, J. Electroanal. Chem. 48, 157 (1973).

    Article  Google Scholar 

  11. P. Yu, M. Pemberton, and P. Plasse, Ptco/C Cathode Catalyst for Improved Durability In PEMFCs, J. Power Sources 144, 11 (2005).

    Article  Google Scholar 

  12. F.T. Wagner, H.A. Gasteiger, R. Makharia, K.C. Neyerlin, E.L. Thompson, and S.G. Yan, Catalyst Development Needs and Pathways for Automotive PEM Fuel Cells, ECS Trans. 3 (1), 19 (2006).

    Article  Google Scholar 

  13. J. Aragane, T. Murahashi, and T. Odaka, Change of Pt Distribution in the Active Components of Phosphoric Acid Fuel Cell, J. Electrochem. Soc. 135, 844 (1988).

    Article  Google Scholar 

  14. J. Aragane, H. Urushibata, and T. Murahashi, Effect of Operational Potential On Performance Decay Rate in a Phosphoric Acid Fuel Cell, J. Appl. Electrochem. 26, 147 (1996).

    Article  Google Scholar 

  15. M. Uchimura and S.S. Kocha, The Impact of Cycle Profile on PEMFC Durability, ECS Trans. 11 (1), 1215 (2007).

    Article  Google Scholar 

  16. S. Mitsushima, Y. Koizumi, S. Uzuka, and K. Ota, Dissolution Mechanism of Platinum in Acidic Media, ECS Trans. 11 (1), 1195 (2007).

    Article  Google Scholar 

  17. P. Yu, W. Gu, R. Makharia, F.T. Wagner, and H.A. Gasteiger, The Impact of Carbon Stability on PEM Fuel Cell Startup and Shutdown Voltage Degradation, ECS Trans. 3 (1), 797 (2006).

    Google Scholar 

  18. H.A. Gasteiger, W. Gu, R. Makharia, M.F. Mathias, and B. Sompalli, “Beginning-of Life MEA Performance - Efficiency Loss Contributions”, in: Handbook of Fuel Cells, edited by W. Vielstich, A. Lamm, and H.A. Gasteiger (Wiley, Chichester, UK, 2003)., vol. 3, pp. 593-610.

    Google Scholar 

  19. M.L. Perry, T.W. Patterson, and C. Reiser, Systems Strategies to Mitigate Carbon Corrosion in Fuel Cells, ECS Trans. 3 (1), 783 (2006).

    Article  Google Scholar 

  20. W. Liu and S. Cleghorn, Effect of Relative Humidity on Membrane Durability in PEM Fuel Cells, ECS Trans. 1 (8), 263 (2006).

    Article  Google Scholar 

  21. E. Endoh, Highly Durable MEA for PEMFC Under High Temperature and Low Humidity Conditions, ECS Trans. 3 (1), 9 (2006).

    Article  MathSciNet  Google Scholar 

Download references

Author information

Authors and Affiliations

Authors

Editor information

Editors and Affiliations

Rights and permissions

Reprints and permissions

Copyright information

© 2008 Springer Science+Business Media B.V

About this paper

Cite this paper

Gasteiger, H.A. et al. (2008). Catalyst Degradation Mechanisms in PEM and Direct Methanol Fuel Cells. In: Kakaç, S., Pramuanjaroenkij, A., Vasiliev, L. (eds) Mini-Micro Fuel Cells. NATO Science for Peace and Security Series C: Environmental Security. Springer, Dordrecht. https://doi.org/10.1007/978-1-4020-8295-5_15

Download citation

  • DOI: https://doi.org/10.1007/978-1-4020-8295-5_15

  • Publisher Name: Springer, Dordrecht

  • Print ISBN: 978-1-4020-8293-1

  • Online ISBN: 978-1-4020-8295-5

  • eBook Packages: EngineeringEngineering (R0)

Publish with us

Policies and ethics