Advertisement

Decoration of domain boundaries: ternary oxides: SrTiO3

  • J. WollschlägerEmail author
Part of the Condensed Matter book series (volume 45B)

Abstract

In this chapter the decoration of domain boundaries in SrTiO3 surface using various methods are discussed in detail.

See Table 66.1.
Table 66.1

SrTiO3

Miller index

Superstructure

Deposit

Sample preparation

Deposition technique

Major experimental techniques

Supporting experimental techniques

Results

Ref.

Fig.

Remarks

(001)

(√5 × √5) R26.6°

Annealing at 1200 °C in UHV

STM

Self-decoration of DB by unknown species

[92Mat]

[93Tan]

[94Mat]

 

Annealing at 1185 °C in UHV

STM

RHEED

Decoration of APDBs and MDBs by Sr and SrO

[97Aki]

 

Annealing at 1200 °C in UHV

NC-AFM

STM

Decoration of APDBs and MDBs by Sr and SrO

[01Kub]

 
Symbols and abbreviations

Short form

Full form

APDB

antiphase domain boundary

RHEED

reflection high-electron energy diffraction

STM

scanning tunneling microscopy

UHV

ultrahigh vacuum

MDB

mirrored domains boundary

NC-AFM

noncontact atomic force microscopy

References

  1. [92Mat]
    Matsumoto, T., Tanaka, H., Kawai, T., Kawai, S.: Surf. Sci. 278, L153 (1992)ADSCrossRefGoogle Scholar
  2. [93Tan]
    Tanaka, H., Matsumoto, T., Kawai, T., Kawai, S.: Jpn. J. Appl. Phys. 32, 1405 (1993)ADSCrossRefGoogle Scholar
  3. [94Mat]
    Matsumoto, T., Tanaka, H., Kouguchi, K., Kawai, T., Kawai, S.: Surf. Sci. 312, 21 (1994)ADSCrossRefGoogle Scholar
  4. [97Aki]
    Akiyama, R., Matsumoto, T., Tanaka, H., Kawai, T.: Jpn. J. Appl. Phys. 36, 3881 (1997)ADSCrossRefGoogle Scholar
  5. [01Kub]
    Kubo, T., Nozoye, H.: Phys. Rev. Lett. 86, 1801 (2001)ADSCrossRefGoogle Scholar

Copyright information

© Springer-Verlag GmbH Germany 2018

Authors and Affiliations

  1. 1.Fachbereich PhysikUniversität OsnabrückOsnabrückGermany

Personalised recommendations