Uniaxial compression tests were conducted on cast and extruded AZ80 alloys at 400 °C and a strain rate of 0.1 s−1 up to a true strain of 1.0. Microstructure and texture evolution during hot deformation was studied using optical microscopy, X-ray diffraction macrotexture analysis and electron backscatter diffraction. The results indicate that dynamic recrystallization (DRX) occurred in the samples during deformation for both cast and extruded starting materials and the DRX fraction was found to increase with deformation strain level. The DRX grain size for both cast and extruded materials was measured as ~5 µm and was independent of the deformation strain. In both cast and extruded materials, hot deformation led to the development of a sharp basal texture along the compression direction, which was attributed to grain rotation occurring during deformation, and preservation of deformation texture by the DRXed grains.

Keywords

Recrystallization texture Cast AZ80 Extruded AZ80 Magnesium DRX EBSD Microstructure evolution Texture evolution Flow stress 

Notes

Acknowledgements

The authors would like to gratefully acknowledge the financial support of the Natural Sciences and Engineering Research Council of Canada (NSERC), Automotive Partnership Canada (APC) program under APCPJ 459269—13 Grant with contributions from Multimatic Technical Centre, Ford Motor Company, and Centerline Windsor. One of the authors (PP) would like to thank Mr. Massimo Di Ciano of University of Waterloo for help in carrying out some of the uniaxial compression tests and Dr. Jian Li and Ms. Renata Zavadil of CanmetMATERIALS for assistance with metallography and EBSD analysis.

References

  1. 1.
    A. A. Luo, “Magnesium: Current and potential automotive applications,” JOM, vol. 54, no. 2, pp. 42–48, 2002.CrossRefGoogle Scholar
  2. 2.
    M. K. Kulekci, “Magnesium and its alloys applications in automotive industry,” The International Journal of Advanced Manufacturing Technology, vol. 39, no. 9, p. 851–865, 2008.CrossRefGoogle Scholar
  3. 3.
    J. Hirsch and T. Al-Samman, “Superior light metals by texture engineering: Optimized aluminum and magnesium alloys for automotive applications,” Acta Materialia, vol. 61, no. 3, pp. 818–843, 2013.CrossRefGoogle Scholar
  4. 4.
    T. Al-Samman and G. Gottstein, “Room temperature formability of a magnesium AZ31 alloy: Examining the role of texture on the deformation mechanisms,” Materials Science and Engineering: A, vol. 488, no. 1–2, pp. 406-414, 2008.CrossRefGoogle Scholar
  5. 5.
    A. Chapuis and J. H. Driver, “Temperature dependency of slip and twinning in plane strain compressed magnesium single crystals,” Acta Materialia, vol. 59, no. 5, pp. 1986–1994, 2011.CrossRefGoogle Scholar
  6. 6.
    T. Al-Samman and G. Gottstein, “Dynamic recrystallization during high temperature deformation of magnesium,” Materials Science and Engineering, vol. 490, no. 1–2, pp. 411–420, 2008.CrossRefGoogle Scholar
  7. 7.
    F. J. Humphreys and M. Hatherly, “Recrystallization of Single-Phase Alloys,” in Recrystallization and Related Annealing Phenomena, Elsevier, 2004, pp. 215–268.Google Scholar
  8. 8.
    Z. Wang, Y. Yang, B. Li, Y. Zhang and Z. Zhang, “Effect of hot-deformation on microstructure and mechanical properties of AZ80 magnesium alloy,” Materials Science and Engineering: A, vol. 582, pp. 36–40, 2013.CrossRefGoogle Scholar
  9. 9.
    D. Toscano, S. K. Shaha, B. Behravesh, H. Jahed and B. Williams, “Effect of Forging on Microstructure, Texture, and Uniaxial Properties of Cast AZ31B Alloy,” Journal of Materials Engineering and Performance, vol. 26, no. 7, p. 3090–3103, 2017.CrossRefGoogle Scholar
  10. 10.
    D. Toscano, S. K. Shaha, B. Behravesh, H. Jahed and B. Williams, “Effect of forging on the low cycle fatigue behavior of cast AZ31B alloy,” Materials Science and Engineering: A, vol. 706, pp. 342–356, 2017.CrossRefGoogle Scholar
  11. 11.
    S. M. H. Karparvarfard, S. K. Shaha, S. B. Behravesh, H. Jahed and B. W. Williams, “Microstructure, texture and mechanical behavior characterization of hot forged cast ZK60 magnesium alloy,” Journal of Materials Science & Technology, vol. 33, no. 9, 2017.CrossRefGoogle Scholar
  12. 12.
    A. Gryguc, S. K. Shaha, S. B. Behravesh, H. Jahed, M. Wells, B. Williams and X. Su, “Monotonic and cyclic behaviour of cast and cast-forged AZ80 Mg,” International Journal of Fatigue, vol. 104, pp. 136–149, 2017.CrossRefGoogle Scholar
  13. 13.
    A. Gryguc, S. B. Behravesh, S. K. Shaha, H. Jahed, M. Wells, B. Williams and X. Su, “Low-cycle fatigue characterization and texture induced ratcheting behaviour of forged AZ80 Mg alloys,” International Journal of Fatigue, vol. 116, pp. 429–438, 2018.CrossRefGoogle Scholar
  14. 14.
    A. Beer and M. Barnett, “Microstructural Development during Hot Working of Mg-3Al-1Zn,” Metallurgical and Materials Transactions A, vol. 38, no. 8, p. 1856–1867, 2007.CrossRefGoogle Scholar
  15. 15.
    M. Shahzad and L. Wagner, “Influence of extrusion parameters on microstructure and texture developments, and their effects on mechanical properties of the magnesium alloy AZ80,” Materials Science and Engineering: A, vol. 506, no. 1–2, pp. 141–147, 2009.CrossRefGoogle Scholar
  16. 16.
    E. I. Poliak and J. J. Jonas, “Initiation of Dynamic Recrystallization in Constant Strain Rate Hot Deformation,” ISIJ International, vol. 43, no. 5, pp. 684–691, 2003.CrossRefGoogle Scholar
  17. 17.
    M. R. Barnett, Z. Kehsavarz, A. G. Beer and D. Atwell, “Influence of grain size on the compressive deformation of wrought Mg–3Al–1Zn,” Acta Materialia, vol. 52, no. 17, pp. 5093–5103, 2004.CrossRefGoogle Scholar
  18. 18.
    X. Yang, H. Miura and T. Sakai, “Dynamic Evolution of New Grains in Magnesium Alloy AZ31 during Hot Deformation,” Materials Transactions, vol. 44, no. 1, pp. 197–203, 2003.CrossRefGoogle Scholar
  19. 19.
    H. Watanabe, H. Tsutsui, T. Mukai, K. Ishikawa, Y. Okanda, M. Kohzu and K. Higashi, “Grain Size Control of Commercial Wrought Mg-Al-Zn Alloys Utilizing Dynamic Recrystallization,” Materials Transactions, vol. 42, no. 7, pp. 1200–1205, 2001.CrossRefGoogle Scholar
  20. 20.
    N. Allain-Bonasso, F. Wagner, S. Berbenni and D. P. Field, “A study of the heterogeneity of plastic deformation in IF steel by EBSD,” Materials Science and Engineering: A, vol. 548, pp. 56–63, 2012.CrossRefGoogle Scholar

Copyright information

© The Minerals, Metals & Materials Society 2019

Authors and Affiliations

  • Paresh Prakash
    • 1
    Email author
  • Amir Hadadzadeh
    • 2
  • Sugrib Kumar Shaha
    • 1
  • Mark A. Whitney
    • 1
  • Mary A. Wells
    • 3
  • Hamid Jahed
    • 1
  • Bruce W. Williams
    • 4
  1. 1.Department of Mechanical and Mechatronics EngineeringUniversity of WaterlooWaterlooCanada
  2. 2.Marine Additive Manufacturing Centre of Excellence (MAMCE)University of New BrunswickFrederictonCanada
  3. 3.College of Engineering and Physical SciencesUniversity of GuelphGuelphCanada
  4. 4.CanmetMATERIALS, Natural Resources CanadaHamiltonCanada

Personalised recommendations