Abstract
The interconnection is determined between the parameters of glass-reinforced plastics formation: the coiling velocity, the emitter voltage drop, and the distance from the rotated envelope surface for the fixed heating temperature.
Similar content being viewed by others
References
Man’ko, T.A., Ermolaev, I.M., Volkov, N.I., Shcheneva, V.B., Solov’ev, A.V., and Ryabovol, A.A., Elektron. Obrab. Mater., 1994, no. 1, pp. 74–75.
Man’ko, T.A., Shcheneva, V.B., Ermolaev, I.M., Volkov, N.I., and Ryabovol, A.A., Tekhn. Mekh., 1997, issue 7, pp. 142–145.
Author information
Authors and Affiliations
Additional information
Original Russian Text © T.A. Man’ko, I.M. Ermolaev, N.I. Volkov, 2007, published in Elektronnaya Obrabotka Materialov, 2007, No. 6, pp. 74–75.
About this article
Cite this article
Man’ko, T.A., Ermolaev, I.M. & Volkov, N.I. Layer-by-layer glass-reinforced plastic formation with application of infrared heating. Surf. Engin. Appl.Electrochem. 43, 472–473 (2007). https://doi.org/10.3103/S1068375507060142
Received:
Issue Date:
DOI: https://doi.org/10.3103/S1068375507060142