Abstract
Changes in the raw materials employed and the coking conditions affect the quality of the tar byproducts used in the production of electrode pitch. The decline in tar quality associated with faster pyrolysis of the vapor-gas products within the coking chamber is discussed. The factors affecting the properties of the newly formed coal tar are analyzed, and the results are compared with theoretical concepts regarding the transformation of the primary products of pyrolysis in the coking chamber. Practical recommendations are developed regarding the production of higher-quality tar. Systematic monitoring of the volume and temperature of the free space within the chamber permits improvement in tar quality, despite increasing coking rates in the production of higher-quality coke. With a tar density of 1185–1190 kg/m3, the moisture content falls to 2.0–5.5%, and the ash content to 0.08–0.11%.
Similar content being viewed by others
References
Kovalev, E.T., Nauchnye osnovy i tekhnologiya pererabotki vysokokipyashchikh fraktsii kamennougol’noi smoly s poluchesniem politsiklicheskikh uglevodorodov (Scientific and Technological Aspects of the Processing of High-Boiling Coal-Tar Fractions to Produce Polycyclic Hydrocarbons), Kharkov: Kontrast, 2001.
Spravochnik koksokhimika. T. 3. Ulavlivanie i pererabotka khimicheskikh produktov koksovaniya (Handbook of Coke Chemistry, Vol. 3: Byproduct Capture and Processing), Kovalev, E.T., Ed., Kharkov: ID INZhEK, 2009.
McHenry, E.R., Industrial pitch quality of the future, Proceedings of the Fourth Australasian Aluminium Smelter Technology Workshop, Sydney, Australia, 1992.
Pityulin, I.N., Nauchno-tekhnologicheskie osnovy sozdaniya kamennougol’nykh uglerodsoderzhashchikh materialov dlya krupnogabaritnykh elektrodov (Scientific and Technological Aspects of the Production of Carbon-Bearing Coal-Tar Materials for Large Electrodes), Kharkov: IPTs Kontrast, 2004.
Mukhina, T.N., Barabanov, N.L., and Babash, S.E., Piroliz uglevodorodnogo syr’ya (Pyrolysis of Hydrocarbon Materials), Moscow: Khimiya, 1987.
Dorofeev, D.S., Miroshnichenko, A.M., and Khadzhinov, V.N., Influence of the coking conditions on the byproduct yield and quality, Koks Khim., 1937, no. 2, pp. 39–44.
Nakagawa, T., Carbon deposition in coke oven chamber: Influence of fine particles on formation rate of carbon deposits, Nippon Steel Technical Report, 2006, no. 7, pp. 63–68.
Baoquan, Z., Achieving good quality tar at Hamilton works, AISI Tech. 2009 Proceedings, 2009, no. 1, pp. 79–88.
Kustov, B.I. and Kolyandr, L.Ya., Koksovyi gaz (Coke-Oven Gas), Kharkov-Moscow: Metallurgizdat, 1947.
Author information
Authors and Affiliations
Corresponding author
Additional information
Original Russian Text © V.N. Rubchevskiy, S.A. Ovchinnikova, V.M. Volokh, R.A. Begma, L.P. Bannikov, V.V. Karchakova, 2014, published in Koks i Khimiya, 2014, No. 4, pp. 33–37.
About this article
Cite this article
Rubchevskiy, V.N., Ovchinnikova, S.A., Volokh, V.M. et al. Influence of coking parameters on the quality of tar for electrode-pitch production. Coke Chem. 57, 158–162 (2014). https://doi.org/10.3103/S1068364X14040061
Received:
Published:
Issue Date:
DOI: https://doi.org/10.3103/S1068364X14040061