Centrifuged fractions, ranging in size from 2·0 to 0·05 µ of a Wyoming bentonite, Bentonita de Durango from Mexico, and Helms clay from Texas were studied. The variation in replacement of Na+, Ca2+, Mg2+, K+, and H+ from these heteroionic clay systems under specific equilibrium conditions of salt concentrations was measured.

The displacement cation distribution was monitored by using specific ion glass electrodes, such as a sodium ion electrode, a cationic glass electrode, a calcium ion electrode and a Tektite electrode. Some factors affecting the exchange reactions are discussed and application of findings to drilling and production techniques is indicated.

Résumé

On a étudié des fractions centrifugées, à dimensions allant de 2,0 à 0,05 µ, d’un bentonite du Wyoming, d’un bentonita de Durango en provenance du Mexique et d’une argile Helms du Texas. On a mesuré la variation du remplacement du Na+, Ca2+, Mg2+, K+ at H+ à partir de ces système d’argile hétéroioniques dans des conditions d’équilibre spécifiques des concentrations du sel.

On a contrôlé la distribution des cations de déplacement en utilisant des électrodes en verre à ion spécifique, p.e. une électrode à ion de sodium, une électrode de verre cationique, une électrode à ion de calcium et une électrode Tektite. On discute certains facteurs relatifs aux réactions d’échange et on indique l’applicabilité des résultats aux techniques de forage et de production.

Kurzreferat

Es wurder zentrifugierte Fraktionen mit einem Grössenbereich von 2, 0 vis 0, 05 µ eines Wyoming Bentonits, Bentonita de Durango aus Mexiko, sowie von Helms Ton aus Texas untersucht. Die Variationen beim Austausch von Na+, Ca2+, Mg2+, K+, und H+ aus diesen hetero-ionischen Tonsystemen wurde unter spezifischen Gleichgewichtsbedingungen der Salzkonzentrationen gemessen.

Die Verdrängungskationenverteilung wurde unter Verwendung spezifischer Ionenglaselktroden, wie z.B. einer Natriumionenelktrode, einer kationischen Glaselektrode, einer Kalziumionenelektrode und einer Tektitelektrode überprüft. Einige der die Austauschreaktionen beeinflussenden Faktoren werden gemeinsam mit der Anwendung der Ergebnisse auf Bohr- und Fördermethoden erörtert.

Резюме

Изучены фракции от 2,0 до 0,06 мк вайомингского бентонита, «бентонита де-Дуранго” (Мексика) и глины из Хелмса (Техас). Установлены вариации замещений Nа+, Са2+. Mg2+, K+ и Н+ в этих гетероионных глинистых системах при определенных равновесных концентрациях солей. Изменение распределения катионов контролировалось с помощью специальных ионных стеклянных электродов, а именно натриевым ионным электродом, катионным стеклянным электродом, кальциевым ионным электродом и электродом Тектайт. Рассматриваются некоторые факторы, оказывающие воздействие на реакции обмена; отмечено значение результатов для техники бурения и технологии.

Preview

Unable to display preview. Download preview PDF.

Unable to display preview. Download preview PDF.

References

  1. Bates, T. F., and Comer, J. J. (1954) Electron Microscopy of Clay Surfaces: Clays and Clay Minerals 3, 1–9.CrossRefGoogle Scholar
  2. Beckman Instruments, Inc., Fullerton, California. Leonard, J. E., Glass Electrodes for Direct Measurement of Sodium Ion Activity in Aqueous Solutions, 1959, Reprint R 6148. Specific Ion Electrodes, Bulletin 7017 A. Fiber Type Reference Electrodes, General Instructions 256A.Google Scholar
  3. Engelhard, W. V., and Tunn, W. (1954) Ueber das Stroemen von Fluessigkeiten durch Sands: Heidelberger Beit. zur Mineral. Petrog. 4, 12–25.Google Scholar
  4. Fertl, W. H., and Jessen, F. W. (1968) Equilibria Studies on Fractionated Natural Clays: Clays and Clay Minerals 16, 313–318.CrossRefGoogle Scholar
  5. Garrels, R. M., and Christ, C. K. (1963) Solution, Minerals and Equilibria: Harper and Row, 450 p.Google Scholar
  6. Grim, R. E. (1953) Clay Mineralogy: McGraw Hill, New York.CrossRefGoogle Scholar
  7. Jackson, M. L. (1967) Lecture series given at the Department of Geology, Spring Semester, The University of Texas, Austin, Texas.Google Scholar
  8. Jessen, F. W., and Mungan, N. (1962) The Effect of Particle Size Distribution and Exchange Cation on Gel Properties of Fractionated Bentonite Suspensions: AIME Petr. Trans. 216, 445–459.Google Scholar
  9. Keithley Instruments, Inc., Cleveland, Ohio, Catalog 1966–1967, pp. 12.Google Scholar
  10. McAtee, J. L. (1958) Heterogeneity in Montmorillonite: Clays and Clay Minerals 5, 279–288.CrossRefGoogle Scholar
  11. Mering, J. (1946) The Hydration of Montmorillonite: Trans. Faraday Soc. 42, 205.CrossRefGoogle Scholar
  12. Monaghan, P. H., et al. (1958) Laboratory Studies of Formation Damage: AIME Fall Meeting, Los Angeles, Calif., 1162–G.Google Scholar
  13. Mungan, N., and Jessen, F. W. (1962) Studies in Fractionated Montmorillonite Suspensions: Clays and Clay Minerals 11, 282–294.CrossRefGoogle Scholar
  14. Pauling, L. (1948) The Nature of Chemical Bond: Cornell University Press, Ithaca, New York, p. 480.Google Scholar
  15. Weiss, A. (1958) Ueber das Kationenaustauschvermoegen der Tonminerale, II. Der Kationenaustausch bei den Mineralen der Glimmer-, Vermikulit und Montmorillonitegruppe: Z. Anorg. Allgem Chem. 297, 257–286.CrossRefGoogle Scholar
  16. Williams, F. J., Neznciyko, M., and Weintritt, D. J. (1953) The Effect of Exchangeable Bases on the Colloidal Properties of Bentonite: J. Phys. Chem. 57, 6.CrossRefGoogle Scholar

Copyright information

© Clay Minerals Society 1969

Authors and Affiliations

  • Walter Fertl
    • 1
  • F. W. Jessen
    • 1
  1. 1.Department of Petroleum EngineeringThe University of TexasAustinUSA

Personalised recommendations