Abstract
A fiber ytterbium laser is used to obtain weakly aggregated nanopowders for yttria-stabilized zirconia solid electrolytes, ZnO and ZnS phosphors, and YAG- and Y2O3-based optical ceramics. The characteristics of the nanopowders are reported. The productivity and energy consumptions of the process with the use of fiber and CO2 lasers are compared. The influence of the buffer gas pressure in the evaporation chamber on the specific surface area of the nanopowder and particle size distribution is studied. The elemental composition of nanoparticles is found to change relative to the composition of the target when yttrium aluminum garnet is evaporated. In the pulsed mode of operation, the energy needed for nanopowder production is minimal when the radiation pulse is about 100 μs long.
Similar content being viewed by others
References
V. V. Osipov, Yu. A. Kotov, M. G. Ivanov, and P. B. Smirnov, Izv. Ross. Akad. Nauk, Ser. Fiz. 63, 1968 (2000).
Yu. A. Kotov, V. V. Osipov, M. G. Ivanov, et al., Zh. Tekh. Fiz. 72(11), 76 (2002) [Tech. Phys. 47, 1420 (2002)].
Yu. A. Kotov, V. V. Osipov, O. M. Samatov, et al., Zh. Tekh. Fiz. 74(3), 72 (2004) [Tech. Phys. 49, 352 (2004)].
F. V. Bunkin and M. I. Tribel’skii, Usp. Fiz. Nauk 130, 193 (1980) [Sov. Phys. Usp. 23, 105 (1980)].
Author information
Authors and Affiliations
Corresponding author
Additional information
Original Russian Text © Yu.A. Kotov, O.M. Samatov, M.G. Ivanov, A.M. Murzakaev, A.I. Medvedev, O.R. Timoshenkova, T.M. Demina, I.V. V’yukhina, 2011, published in Zhurnal Tekhnicheskoĭ Fiziki, 2011, Vol. 81, No. 5, pp. 65–68.
Rights and permissions
About this article
Cite this article
Kotov, Y.A., Samatov, O.M., Ivanov, M.G. et al. Production and characteristics of composite nanopowders using a fiber ytterbium laser. Tech. Phys. 56, 652–655 (2011). https://doi.org/10.1134/S1063784211050173
Received:
Published:
Issue Date:
DOI: https://doi.org/10.1134/S1063784211050173