Abstract
New lithium-conducting solid solutions based on lithium orthozirconate have been synthesized by mutual doping of the related structures Li8ZrO6 and Li7NbO6. The main factor determining the increase in the electrical conductivity of the Li8 − x Zr1 − x Nb x O6 solid solutions is the formation of lithium vacancies in the tetrahedral and octahedral layers. The practical stability of the Li8 − x Zr1 − x Nb x O6 ceramics to metallic lithium has been studied.
Similar content being viewed by others
References
O. L. Andreev, N. N. Batalov, and T. V. Sofronova, Elektrokhim. Energ., No. 2, 61 (2002).
C. Muhle, R. E. Dinnebier, L. Wullen, G. Schwering, and M. Jansen, Inorg. Chem. 43, 874 (2004).
Joint Committee on Powder Diffraction Standards— International Centre for Diffraction Data (JCPDS- ICDD, Newtown Square, Pennsylvania, United States, 1986).
M. I. Pantyukhina, O. L. Andreev, B. D. Antonov, and N. N. Batalov, Russ. J. Inorg. Chem. 47(11), 1630 (2002).
Author information
Authors and Affiliations
Corresponding author
Additional information
Original Russian Text © M.I. Pantyukhina, M.S. Shchelkanova, S.V. Plaksin, 2013, published in Fizika Tverdogo Tela, 2013, Vol. 55, No. 4, pp. 650–651.
Rights and permissions
About this article
Cite this article
Pantyukhina, M.I., Shchelkanova, M.S. & Plaksin, S.V. Synthesis and electrochemical properties of Li8 − x Zr1 − x Nb x O6 solid solutions. Phys. Solid State 55, 707–709 (2013). https://doi.org/10.1134/S1063783413040227
Received:
Published:
Issue Date:
DOI: https://doi.org/10.1134/S1063783413040227