Abstract
The use of natural halloysite clay tubes 50 nm in diameter as nanocontainers for loading, storing, and slowly releasing organic corrosion inhibitors is described. Loaded nanotubes can be mixed well with many polymers and dyes in amounts of 5–10 wt % to form a ceramic framework (which increases the strength of halloysite composites by 30–50%), increase the adhesion of these coatings to metals, and allow for the slow release of corrosion inhibitors in defects of coatings. A significant improvement of protective anticorrosion properties of polyacryl and polyurethane coatings containing ceramic nanotubes loaded with benzotriazole and hydroxyquinoline is demonstrated.
This is a preview of subscription content, access via your institution.
References
E. Joussein, S. Petit, J. Churchman, et al., Clay Miner. 40, 383 (2005).
Y. Lvov, D. Shchukin, H. Möhwald, et al., ACS Nano 2, 814 (2008).
M. Du, B. Guo, and D. Jia, Polymer Intern. 59, 574 (2010).
Y. Lvov and E. Abdullayev, Progress Polymer Sci. 38, 1690 (2013).
E. Abdullayev, V. Abbasov, A. Tursunbayeva, et al., ACS Appl. Mater. Surf. 5, 4464 (2013).
E. Abdullayev and Y. Lvov, J. Mater. Chem. B 1, 2894 (2013).
E. Abdullayev, A. Joshi, W. Wei, et al., ACS Nano 6, 7216 (2012).
W-O. Yah, A. Takahara, and Y. Lvov, J. Am. Chem. Soc. 134, 1853 (2012).
X. Lai, M. Agarwal, Y. Lvov, et al., J. Appl. Toxicity 33, 1316 (2013).
V. Vergaro, E. Abdullayev, R. Cingolani, et al., Biomacromol. 11, 820 (2010).
Y. Zhang, Y. Chen, H. Zhang, et al., J. Inorg. Biochem. 118, 59 (2013).
D. Shchukin and H. Möhwald, Small 3, 926 (2007).
F. Presuel-Moreno, M. Jakab, N. Tailleart, et al., Mater. Today 11, 14 (2008).
H. Kelly, P. Deasy, E. Ziaka, et al., Int. J. Pharm. 274, 167 (2004).
Y. Lvov, A. Aerov, and R. Fakhrullin, Adv. Colloid Interface Sci. 201, 1287 (2013).
E. Abdullayev, K. Sakakibara, K. Okamoto, et al., ACS Appl. Mater. Interf. 3, 4040 (2011).
K. Babic-Samardzija and N. Hackerman, J. Solid State Electrochem. 9, 483 (2005).
B. Guo, Y. Lei, F. Chen, et al., Appl. Surf. Sci. 7, 188 (2008).
B. Guo, Q. Zou, Y. Lei, et al., New Chem. Mater. 36, 32 (2008).
M. Liu, B. Guo, M. Du, et al., Nanotechnology 18, 455703 (2007).
M. Du, B. Guo, and D. Jia, Eur. Polym. J. 42, 1362 (2006).
G. Cavallaro, G. Lazzara, S. Milioto, et al., Langmuir 27, 1158 (2011).
M. Liu, C. Wu, Y. Jiao, et al., J. Mater. Chem. B 1, 2078 (2013).
Z. Huang, Z. Jia, B. Guo, et al., China Plast. Ind. 36, 29 (2008).
D. Fix, D. Andreeva, H. Möhwald, et al., Adv. Funct. Mater. 19, 1720 (2009).
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Fakhrullin, R.F., Tursunbayeva, A., Portnov, V.S. et al. Ceramic nanotubes for polymer composites with stable anticorrosion properties. Crystallogr. Rep. 59, 1107–1113 (2014). https://doi.org/10.1134/S1063774514070104
Received:
Published:
Issue Date:
DOI: https://doi.org/10.1134/S1063774514070104
Keywords
- Polymer Composite
- Crystallography Report
- Corrosion Inhibitor
- Dodecylamine
- Anticorrosion Property