Abstract
In order to improve the thermal properties of coke, an industrial experiment on the coke spraying with ZBS additive solution was carried out at coking plant and No. 6 blast furnace (2 000 m3) of Kunming Iron and Steel Co Ltd. The coke reaction index (CRI) of the coke spraying with ZBS additive solution decreases by 10. 56%. and the coke strength after reaction (CSR) increases by 7.80% in comparison with those of the un-sprayed coke. During the experiment, the average iron output increases by 66. 69 t/d, and the coke rate is reduced by 5.21 kg per ton iron, while the fluctuation of furnace temperture is small, and sulphur content in hot metal and 100% of hot metal are acceptable.
Similar content being viewed by others
References
YANG Jie-kang. Analysis of Hot Properties of Ironmaking Coke at Kunming Iron and Steel Company [J]. Journal of Bao-tou University of Iron and Steel Technology, 1999, 18(Sup): 291–293 (in Chinese).
CUI Ping, QIAN Zhuan-fen, YANG Jun-he. Quality Assessment of Metallurgical Coke [J]. Iron and Steel, 2000, 35(6): 1–4 (in Chinese).
ZHU Zi-zong, SHEN Yong-ling, MIAO Tie-ling, et al. Industrial Experiment on Improving Coke Thermal Properties at Anyang Iron and Steel Co Ltd [J]]. Iron and Steel, 2004, 39(2): 5–7 (in Chinese).
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Zhu, Zz., Zhang, Zm., Tang, Qy. et al. Industrial Experiment on Coke Spraying With ZBS Additive in Blast Furnace. J. Iron Steel Res. Int. 13, 14–17 (2006). https://doi.org/10.1016/S1006-706X(06)60053-8
Revised:
Published:
Issue Date: