Abstract
In this study the corrosion, sedimentation and subsequently choking in the air cooler tubes of benzene drying section in Bistoun Petrochemical Company, at Iran were investigated. The main reasons of failure were analyzed using standard failure analysis techniques such as visual checking, chemical and mechanical characterizations, metallurgical examinations employing optical microscopy in combination with scanning electron microscopy, X-ray fluorescence and X-ray diffraction analysis. The chemical analysis was used to determine the corrosion products. The accumulation of sediment and under-deposit corrosion has resulted in localized corrosion and perforation in the inner surface of the tubes. In addition, the erosion–corrosion accelerated the destruction of tubes. The microbial corrosion can happen because of high water content. The results showed that a combination of corrosion types has occurred. A new idea was proposed for the separation mechanism of low concentration of water from benzene in the process. Finally, the suggestions have been proposed for trouble shooting, preventing corrosion and clogging in the tubes of air cooler and subsequently avoiding production stop.
Similar content being viewed by others
References
Allahkaram SR, Zakersafaee P, Haghgoo SAM (2011) Failure analysis of heat exchanger tubes of four gas coolers. Eng Fail Anal 18:1108–1114. https://doi.org/10.1016/j.engfailanal.20
Blackburn FE (2004) Non-bioassay techniques for monitoring MIC, paper 04580. CORROSION, NACE International, Houston
Burstein G, Sasaki K (2000) Effect of impact angle on the slurry erosion–corrosion of 304 L stainless steel. Wear 240:80–94
Deport R, Hero HM (1944) The Nalco guide to boiler failure analysis. Hill Inc., Philadelphia
Feller D (1999) Strength of the benzene–water hydrogen bond. J Phys Chem A 103:7558–7561
Furutaka S, Ikawa S (2002) π-hydrogen bonding between water and aromatic hydrocarbons at high temperatures and pressures. J Chem Phys 117:751–755. https://doi.org/10.1063/1.475953
Ghanbarian M, Nabizadeh R, Mahvi AH, Nasseri S, Naddafi K (2011) Photocatalytic degradation of linear alkyl benzene sulfonate from aqueous solution by TiO2 nanoparticles. Iran J Environ Health Sci Eng 8:309–316
Gierszal KP, Davis JG, Hands MD, Wilcox DS, Slipchenko LV, Amotz DB (2011) π-hydrogen bonding in liquid water. J Phys Chem Lett 2:2930–2933. https://doi.org/10.1021/jz201373e
Herro HM, Port RD (1993) The Nalco guide to cooling water system failure analysis. McGraw-Hill, New York City
Hu SM, Wang SH, Yang ZG (2015) Failure analysis on unexpected wall thinning of heat-exchange tubes in ammonia evaporators, case studies. Eng Fail Anal 3:52–61. https://doi.org/10.1016/j.csefa.2015.01.002
Huang J (2013) Mechanistic study of under deposit corrosion of mild steel in aqueous carbon dioxide solution. Russ College of engineering and technology, Ohio University, Ohio
Javaherdashti R (2008) Microbiologically influenced corrosion: an engineering insight. Springer, London
Kermani M, Morshed A (2003) Carbon dioxide corrosion in oil and gas production—a compendium. Corrosion 59:659–683. https://doi.org/10.5006/1.3277596
Khajavi MR, Abdolmaleki AR, Adibi N, Mirfendereski S (2007) Failure analysis of bank front boiler tubes. Eng Fail Anal 14:731–738. https://doi.org/10.1016/j.engfailanal.2005.10.017
Lee H, Lee H, Kim HE, Kweon J, Lee BD, Lee C (2014) Oxidant production from corrosion of nano- and micro particulate zero-valent iron in the presence of oxygen: a comparative study. J Hazard Mater 265:201–207. https://doi.org/10.1016/j.jhazmat.2013.11.066
Little BJ, Lee JS (2007) microbiologically influenced corrosion. Wiley, Hoboken
Lu Y, Wang J, Yu L, Kovarik L, Zhang X, Hoffman AS, Gallo A, Bare SR, Sokaras D, Kroll T, Dagle V, Xin H, Karim AM (2019) Identification of the active complex for CO oxidation over single-atom Ir–on–MgAl2O4 catalysts. Nat Catal 2:149–156. https://doi.org/10.1038/s41929-018-0192-4
Malka R, Nesic S, Gulino DA (2007) Erosion–corrosion and synergistic effects in disturbed liquid-particle flow. Wear 262:791–799. https://doi.org/10.1016/j.wear.2006.08.029
Nakahara M, Wakai C (1992) Monomeric and cluster states of water molecules in organic solvent. Chem Lett 21:809–812. https://doi.org/10.1246/cl.1992.809
Nasirpouri F, Mostafaei A, Fathyunes L, Jafari R (2014) Assessment of localized corrosion in carbon steel tube-grade AISI 1045 used in output oil–gas separator vessel of desalination unit in oil refinery industry. Eng Fail Anal 40:75–88. https://doi.org/10.1016/j.engfailanal.2014.02.012
Neville A, Hodgkiess T (1997) Study of effect of liquid corrosivity in liquid-solid impingement on cast iron and austenitic stainless steel. Br Corros J 32:197–205. https://doi.org/10.1179/000705997798114904
Pandey RK (2006) Failure analysis of refinery tubes of overhead condenser. Eng Fail Anal 13:739–746. https://doi.org/10.1016/j.engfailanal.2005.02.016
Rawat J, Khandelwal A, Sharma N, Tyagi S (2016) Effect of Sulphate reducing bacterial–biofilm isolated from refinery cooling water system and sonication on corrosion of carbon steel. J Mater Environ Sci 7(2):596–604
Selvam K, Ayyagari A, Grewal HS, Mukherjee S, Aror HS (2017) Enhancing the erosion–corrosion resistance of steel through friction stir processing. Wear 386–387:129–138. https://doi.org/10.1016/j.wear.2017.06.009
Slipchenko LV, Gordon MS (2009) Water–benzene interactions: an effective fragment potential and correlated quantum chemistry study. J Phys Chem A 113:2092–2102. https://doi.org/10.1021/jp808845b
Sridhar N, Dunn D, Anderko A, Lencka M, Schutt H (2001) Effects of water and gas compositions on the internal corrosion of gas pipelines—modeling and experimental studies. Corrosion 57:221–235. https://doi.org/10.5006/1.3290347
Virk MA, Butt MA, Chughtai A, Ahmad M, Khan IH, Deen KM (2010) Failure analysis of heat exchanger fluid vapour phase vent lines in a Polyester plant. Eng Fail Anal 17:447–454. https://doi.org/10.1016/j.engfailanal.2009.09.005
Watson S, Friedersdorf F, Madsen B, Cramer S (1995) Methods of measuring wear-corrosion synergism. Wear 181:476–484. https://doi.org/10.1016/0043-1648(95)90161-2
Manual and document of alkylation unit of Bistoun Petrochemical Company in Iran
Zhou S, Stack M, Newman R (1996) Characterization of synergistic effects between erosion and corrosion in an aqueous environment using electrochemical techniques. Corrosion 52:934–946. https://doi.org/10.5006/1.3292087
Zhu M, Ou G, Jin H, Wang K, Zheng Z (2015) Top of the REAC tube corrosion induced by under deposit corrosion of ammonium chloride and erosion corrosion. Eng Fail Anal 57:483–489. https://doi.org/10.1016/j.engfailanal.2015.08.022
Acknowledgements
The author is grateful to thank Mr Amjad Sorourian, Hadi Azami and Kambiz Ghasemi from Bistoun Petrochemical Company for their technical guidance.
Author information
Authors and Affiliations
Corresponding author
Additional information
Publisher's Note
Springer Nature remains neutral with regard to jurisdictional claims in published maps and institutional affiliations.
Rights and permissions
About this article
Cite this article
Shokri, A. An investigation of corrosion and sedimentation in the air cooler tubes of benzene drying column in linear alkyl benzene production plant. Chem. Pap. 73, 2265–2274 (2019). https://doi.org/10.1007/s11696-019-00776-z
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s11696-019-00776-z