This case study demonstrates that Alloy 601 (UNS N06601) is susceptible to strain-age cracking. The observation illustrates the potential importance of post weld heat treatment to the successful utilization of this alloy in certain applications.

Keywords

Stress Relaxation Failure Analysis Post Weld Heat Treatment Reformer Practical Failure Analysis Volume 